(Viewing data as-entered.
Click here
to return)
Garlock 7164 SBR Rubber Lining
Categories:
Polymer
;
Thermoset
;
Rubber or Thermoset Elastomer (TSE)
;
Styrene Butadiene Rubber
Material Notes:
SBR rubber lining for protection applications such as chute lining and skirtboards.
An optional duck fabric backing is available.
Information provided by Garlock Rubber Technologies
Key Words:
ASTM D2000-BA-620
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Mechanical Properties
Original Value
Comments
Hardness, Shore A
55 - 65
Tensile Strength
>=
2000
psi
2400
psi
Typical
Elongation at Break
>= 300 %
Thermal Properties
Original Value
Comments
Maximum Service Temperature, Air
200
°F
Minimum Service Temperature, Air
-20.0
°F
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to go back to viewing the property data in MatWeb's normal format.
Users viewing this material also viewed the following:
BASF D 2000 Polyetheramine
Garlock 244 Neoprene Rubber - Commercial Grade
Natural Rubber, Vulcanized (NR, IR, Polyisoprene)
Rubatex R421 Neoprene/EPDM/SBR Rubber Foam Sheet
LG Chemical SBR 1500H High Acrylonitrile Polymer
PGARL982 / 157455
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.