MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Celanese Celanex® 3200-2FC PBT, 15% Glass Reinforced
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT); Polybutylene Terephthalate (PBT), 20% Glass Fiber Filled

Material Notes: Celanex 3200-2FC is a general purpose, 15% glass reinforced polybutylene terephthalate with a good balance of mechanical properties and processability for use in food contact applications. Celanex 3200-2FC contains an internal lubricant.

Information provided by Celanese

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.41 g/cc1.41 g/ccASTM D792
Density 1.41 g/cc0.0509 lb/in³ISO 1183
Moisture Absorption 0.200 %0.200 %23°C/50%RH; ISO 62
Linear Mold Shrinkage, Flow 0.0050 - 0.0070 cm/cm0.0050 - 0.0070 in/inISO 294-4
 0.0050 - 0.0070 cm/cm0.0050 - 0.0070 in/inASTM D955
Melt Flow 26 g/10 min26 g/10 minASTM D1238
 26 g/10 min
@Load 2.16 kg,
Temperature 250 °C
26 g/10 min
@Load 4.76 lb,
Temperature 482 °F
[cm3/10min]; ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 9090ISO 2039-2
Tensile Strength at Break 93.1 MPa13500 psiASTM D638
 100 MPa14500 psi5mm/min; ISO 527-2/1A
 44.8 MPa
@Temperature 121 °C
6500 psi
@Temperature 250 °F
ASTM D638
 55.2 MPa
@Temperature 80.0 °C
8000 psi
@Temperature 176 °F
ASTM D638
 105 MPa
@Temperature 0.000 °C
15200 psi
@Temperature 32.0 °F
ASTM D638
 108 MPa
@Temperature -40.0 °C
15700 psi
@Temperature -40.0 °F
ASTM D638
Elongation at Break 3.0 %3.0 %ASTM D638
 3.5 %3.5 %5mm/min; ISO 527-2/1A
 1.9 %
@Temperature 4.44 °C
1.9 %
@Temperature 40.0 °F
ASTM D638
 2.0 %
@Temperature 0.000 °C
2.0 %
@Temperature 32.0 °F
ASTM D638
 6.3 %
@Temperature 80.0 °C
6.3 %
@Temperature 176 °F
ASTM D638
 6.3 %
@Temperature 121 °C
6.3 %
@Temperature 250 °F
ASTM D638
Tensile Modulus 5.52 GPa800 ksiASTM D638
 5.80 GPa841 ksi50mm/min; ISO 527-2/1A
 2.07 GPa
@Temperature 121 °C
300 ksi
@Temperature 250 °F
ASTM D638
 2.45 GPa
@Temperature 80.0 °C
355 ksi
@Temperature 176 °F
ASTM D638
 6.21 GPa
@Temperature 0.000 °C
900 ksi
@Temperature 32.0 °F
ASTM D638
 6.41 GPa
@Temperature -40.0 °C
930 ksi
@Temperature -40.0 °F
ASTM D638
Flexural Strength 145 MPa21000 psiASTM D790
 150 MPa21800 psiISO 178
Flexural Modulus 4.83 GPa700 ksiASTM D790
 5.20 GPa754 ksiISO 178
Izod Impact, Notched 0.534 J/cm1.00 ft-lb/inASTM D256
Izod Impact, Notched (ISO) 5.00 kJ/m²2.38 ft-lb/in²ISO 180/1A
Charpy Impact Unnotched 2.00 J/cm²9.52 ft-lb/in²ISO 179/1eU
 2.00 J/cm²
@Temperature -30.0 °C
9.52 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eU
Charpy Impact, Notched 0.550 J/cm²2.62 ft-lb/in²ISO 179/1eA
 0.500 J/cm²
@Temperature -30.0 °C
2.38 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+15 ohm-cm>= 1.00e+15 ohm-cmIEC 60093
 1.00e+16 ohm-cm1.00e+16 ohm-cmASTM D257
Surface Resistance >= 1.00e+15 ohm>= 1.00e+15 ohmIEC 60093
Dielectric Constant  3.5
@Frequency 1e+6 Hz
3.5
@Frequency 1e+6 Hz
ASTM D150
 3.8
@Frequency 1e+6 Hz
3.8
@Frequency 1e+6 Hz
IEC 60250
 4.2
@Frequency 100 Hz
4.2
@Frequency 100 Hz
IEC 60250
Dielectric Strength 18.1 kV/mm460 kV/inshort term; ASTM D149
 29.0 kV/mm737 kV/inIEC 60243-1
Dissipation Factor  0.0010
@Frequency 1e+6 Hz
0.0010
@Frequency 1e+6 Hz
ASTM D150
 0.0016
@Frequency 100 Hz
0.0016
@Frequency 100 Hz
IEC 60250
 0.020
@Frequency 1e+6 Hz
0.020
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index 350 V350 VIEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 40.0 µm/m-°C22.2 µin/in-°FISO 11359-2
CTE, linear, Transverse to Flow 110 µm/m-°C61.1 µin/in-°FISO 11359-2
Melting Point 225 °C437 °F10°C/min; ISO 11357-1,-2,-3
 225 °C437 °FASTM D3418
Deflection Temperature at 0.46 MPa (66 psi) 213 °C415 °FASTM D648
 215 °C419 °FISO 75-1, -2
Deflection Temperature at 1.8 MPa (264 psi) 192 °C378 °FASTM D648
 195 °C383 °FISO 75-1, -2
Deflection Temperature at 8.0 MPa 90.0 °C194 °FISO 75-1, -2
Vicat Softening Point 215 °C419 °FISO 306
Glass Transition Temp, Tg 60.0 °C140 °FISO 11357-1,-2,-3
Flammability, UL94 HB
@Thickness 0.710 mm
HB
@Thickness 0.0280 in
Oxygen Index 20 %20 %ISO 4589
 
Processing PropertiesMetricEnglishComments
Processing Temperature 65.0 - 93.0 °C149 - 199 °Fcavity
 250 - 260 °C482 - 500 °Fhot runner
Feed Temperature 230 - 240 °C446 - 464 °F
Zone 1 230 - 240 °C446 - 464 °F
Zone 2 235 - 250 °C455 - 482 °F
Zone 3 235 - 250 °C455 - 482 °F
Zone 4 240 - 260 °C464 - 500 °F
Die Temperature 250 - 260 °C482 - 500 °F
Melt Temperature 235 - 260 °C455 - 500 °F
 260 °C500 °FISO 294
Mold Temperature 82.0 °C180 °FISO 294
Injection Velocity 300 mm/sec11.8 in/secISO 294
Drying Temperature 120 - 130 °C248 - 266 °F
Dry Time 4.00 hour4.00 hour
Moisture Content <= 0.020 %<= 0.020 %
Hold Pressure 48.0 MPa6960 psiISO 294
 
Descriptive Properties
Injection moldingYes
Injection speedmedium-fast
Processing conditions acc. ISO7792-2

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Celanese Celanex® 3300D PBT, 30% Glass Reinforced
Celanese Celanex® 2000-3FC PBT, Unfilled
Celanese Celanex® 3300-2FC PBT, 30% Glass Reinforced
Celanese Celanex® 2002-2 PBT, Unfilled
Celanese Celanex® 2001FC PBT, Unfilled

PHCQ040 / 178495

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.