MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Mitsubishi Xantar® C CP 200 Polycarbonate
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate, Molded

Material Notes: XANTAR® C properties are: Highest flow in combination with excellent toughness. High level of purity. High stability. Bright natural color. The benefits are: easier filling of complex parts, lower mould deposit during injection molding, low volatiles level and reduced fogging tendency, better long-term property retention and improved color consistency and appearance.

Information provided by Mitsubishi Engineering Plastics Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.10 g/cc0.0397 lb/in³
Water Absorption 0.70 %0.70 %
Moisture Absorption 0.200 %0.200 %
Linear Mold Shrinkage, Flow 0.0060 cm/cm0.0060 in/in
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 45.0 MPa6530 psi
Elongation at Break >= 50 %>= 50 %
Elongation at Yield 4.5 %4.5 %
Tensile Modulus 2.00 GPa290 ksi
Flexural Strength 67.0 MPa9720 psi
Flexural Modulus 1.80 GPa261 ksi
Izod Impact, Notched (ISO) 50.0 kJ/m²
@Temperature 23.0 °C
23.8 ft-lb/in²
@Temperature 73.4 °F
Charpy Impact Unnotched  NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
 NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+15 ohm-cm>= 1.00e+15 ohm-cm
Surface Resistance 1.00e+15 ohm1.00e+15 ohm
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 90.0 µm/m-°C50.0 µin/in-°F
CTE, linear, Transverse to Flow 90.0 µm/m-°C50.0 µin/in-°F
Deflection Temperature at 1.8 MPa (264 psi) 95.0 °C203 °F
Vicat Softening Point 112 °C
@Load 5.10 kg
234 °F
@Load 11.2 lb
rate 50°C/h
 
Processing PropertiesMetricEnglishComments
Melt Temperature 260 °C500 °FAs Tested; Injection
Mold Temperature 80.0 °C176 °FAs Tested; Injection

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Covestro Bayblend® T45 PG Polycarbonate + ABS

PMITSU9344 / 192008

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.