MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Covestro Bayblend® T45 PG Polycarbonate + ABS
Categories: Polymer; Thermoplastic; ABS Polymer; Polycarbonate/ABS Alloy, Unreinforced; Polycarbonate (PC)

Material Notes: ABS+PC-Blend; Vicat/B 120 temperature = 112 °C; for electroplating applications

As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covestro.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.10 g/cc0.0397 lb/in³ISO 1183
Moisture Absorption at Equilibrium 0.20 %0.20 %ISO 62
Water Absorption at Saturation 0.70 %0.70 %ISO 62
Viscosity 200000 cP
@Shear Rate 1000 1/s,
Temperature 260 °C
200000 cP
@Shear Rate 1000 1/s,
Temperature 500 °F
b.o. ISO 11443-A
Linear Mold Shrinkage, Flow 0.0055 - 0.0075 cm/cm
@Thickness 3.00 mm
0.0055 - 0.0075 in/in
@Thickness 0.118 in
150x105x3 mm; 260 °C / MT 80 °C; b.o. ISO 2577
Linear Mold Shrinkage, Transverse 0.0055 - 0.0075 cm/cm
@Thickness 3.00 mm
0.0055 - 0.0075 in/in
@Thickness 0.118 in
150x105x3 mm; 260 °C / MT 80 °C; b.o. ISO 2577
Melt Flow 12 g/10 min
@Load 5.00 kg,
Temperature 260 °C
12 g/10 min
@Load 11.0 lb,
Temperature 500 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 40.0 MPa5800 psi50 mm/min; ISO 527-1/-2
Tensile Strength, Yield 49.0 MPa7110 psi50 mm/min; ISO 527-1/-2
Elongation at Break >= 50 %>= 50 %50 mm/min; ISO 527-1/-2
Elongation at Yield 3.7 %3.7 %50 mm/min; ISO 527-1/-2
Tensile Modulus 2.10 GPa305 ksi1 mm/min; ISO 527-1/-2
Izod Impact, Notched (ISO)  36.0 kJ/m²
@Temperature -30.0 °C
17.1 ft-lb/in²
@Temperature -22.0 °F
ISO 180-A
 40.0 kJ/m²
@Temperature 23.0 °C
19.0 ft-lb/in²
@Temperature 73.4 °F
ISO 180-A
Izod Impact, Unnotched (ISO)  NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
ISO 180-U
 NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
ISO 180-U
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+14 ohm-cm1.00e+14 ohm-cmIEC 60093
Surface Resistance 1.00e+16 ohm1.00e+16 ohmIEC 60093
Dielectric Constant  3.0
@Frequency 1e+6 Hz
3.0
@Frequency 1e+6 Hz
IEC 60250
 3.1
@Frequency 100 Hz
3.1
@Frequency 100 Hz
IEC 60250
Dielectric Strength 35.0 kV/mm889 kV/in1 mm; IEC 60243-1
Dissipation Factor  0.0035
@Frequency 100 Hz
0.0035
@Frequency 100 Hz
IEC 60250
 0.0085
@Frequency 1e+6 Hz
0.0085
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index 275 V275 VSolution A; IEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 85.0 µm/m-°C
@Temperature 23.0 - 55.0 °C
47.2 µin/in-°F
@Temperature 73.4 - 131 °F
ISO 11359-1,-2
CTE, linear, Transverse to Flow 90.0 µm/m-°C
@Temperature 23.0 - 44.0 °C
50.0 µin/in-°F
@Temperature 73.4 - 111 °F
ISO 11359-1,-2
Thermal Conductivity 0.142 W/m-K0.985 BTU-in/hr-ft²-°FMelt
Deflection Temperature at 0.46 MPa (66 psi) 112 °C234 °FISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 95.0 °C203 °FISO 75-1/-2
Vicat Softening Point  110 °C
@Load 5.10 kg
230 °F
@Load 11.2 lb
50°C/h; ISO 306
 112 °C
@Load 5.10 kg
234 °F
@Load 11.2 lb
120°C/h; ISO 306
Flammability, UL94 HB
@Thickness 0.850 mm
HB
@Thickness 0.0335 in
IEC 60695-11-10
 
Processing PropertiesMetricEnglishComments
Melt Temperature 260 °C500 °FInjection Molding; ISO 294
Mold Temperature 80.0 °C176 °FInjection Molding; ISO 294
Injection Velocity 240 mm/sec9.45 in/secISO 294

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Covestro Bayblend® 2953 Polycarbonate + ABS Blend, Automotive Plating
Covestro Bayblend® T65 HI PC/ABS Blend
Covestro Bayblend® KU 1-1446 Polycarbonate + ABS
Covestro Bayblend® T65 XF Polycarbonate + ABS
Mitsubishi Xantar® C CP 200 Polycarbonate

PB09732 / 92572

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.