MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Covestro Bayblend® 2953 Polycarbonate + ABS Blend, Automotive Plating
Categories: Polymer; Thermoplastic; ABS Polymer; Polycarbonate/ABS Alloy, Unreinforced; Polycarbonate (PC)

Material Notes: (PC+ABS)-Blend; Vicat/B 120 temperature = 113°C; for electroplating applications

As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covestro.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.11 g/cc0.0401 lb/in³ISO 1183-1
Melt Flow 15.5 g/10 min
@Load 5.00 kg,
Temperature 260 °C
15.5 g/10 min
@Load 11.0 lb,
Temperature 500 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 47.0 MPa6820 psi50 mm/min; ISO 527-1,-2
Tensile Strength, Yield 44.0 MPa6380 psi50 mm/min; ISO 527-1,-2
Elongation at Break >= 50 %>= 50 %50 mm/min; ISO 527-1,-2
Elongation at Yield 3.6 %3.6 %50 mm/min; ISO 527-1,-2
Tensile Modulus 2.10 GPa305 ksi1 mm/min; ISO 527-1,-2
Flexural Strength 448 MPa
@Strain 3.5 %
65000 psi
@Strain 3.5 %
2 mm/min; ISO 178
Flexural Modulus 2.20 GPa319 ksi2 mm/min; ISO 178
Flexural Strain at Break 5.6 %5.6 %2 mm/min; ISO 178
Izod Impact, Notched (ISO)  35.0 kJ/m²
@Temperature -30.0 °C
16.7 ft-lb/in²
@Temperature -22.0 °F
ISO 180-A
 46.0 kJ/m²
@Temperature 23.0 °C
21.9 ft-lb/in²
@Temperature 73.4 °F
ISO 180-A
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 110 °C230 °FISO 75-1,-2
Deflection Temperature at 1.8 MPa (264 psi) 90.0 °C194 °FISO 75-1,-2
Vicat Softening Point  108 °C
@Load 5.10 kg
226 °F
@Load 11.2 lb
50°C/h; ISO 306
 113 °C
@Load 5.10 kg
235 °F
@Load 11.2 lb
120°C/h; ISO 306

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Covestro Bayblend® T45 PG Polycarbonate + ABS
Parker Chomerics ECOPLATE™ 5030
A. Schulman Diamond ABSPC 8901P ABS/PC Plating Grade, High Impact
Chi Mei Polylac® PA-727 ABS
Cossa Polimeri ESTADIENE CR 1 Acrylonitrile Butadiene Styrene

PB1B04 / 26397

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.