MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Morgan Advanced Ceramics SSN Sintered Silicon Nitride Mac-SSNS
Categories: Ceramic; Nitride

Material Notes: An advanced synthetic ceramic with a nominal Si3N4 content of 99%. The sintered silicon nitride (SSN) technique produces a material with excellent physical properties that is ideally suited to components that operate under thermally demanding conditions.

Prime Features:

  • Outstanding resistance to thermal downshock
  • Extremely hard and wear resistant
  • .Exceptional compressive strength
  • Excellent resistance to attack from molten non-ferrous alloys containing aluminium, magnesium, copper, zinc and lead
  • Spatter resistant
  • Low thermal conductivity
  • High electrical resistivity
Typical Applications:
  • Shrouds for TIG/MIG welding torches
  • Shrouds for plasma cutting torches
  • Heat treatment jigs and fixtures
  • Bearing balls and rollers
Production Capabilities:
  • Manufacture to close engineering tolerances
  • Prototype, batch and volume production

Information provided by Morgan Advanced Materials

Key Words: SSN
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 3.20 g/cc0.116 lb/in³fired
Open Porosity 0.00 %0.00 %fully dense, nominal, apparent
 
Mechanical PropertiesMetricEnglishComments
Hardness, Vickers 16
@Load 0.500 kg
16
@Load 1.10 lb
[Gpa]
Modulus of Elasticity 280 GPa
@Temperature 20.0 °C
40600 ksi
@Temperature 68.0 °F
Flexural Strength 650 MPa
@Temperature 20.0 °C
94300 psi
@Temperature 68.0 °F
3 point
Compressive Strength >= 3000 MPa>= 435000 psi
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+12 ohm-cm
@Temperature 20.0 °C
>= 1.00e+12 ohm-cm
@Temperature 68.0 °F
pure form
 
Thermal PropertiesMetricEnglishComments
CTE, linear 8.80 µm/m-°C
@Temperature 20.0 - 1000 °C
4.89 µin/in-°F
@Temperature 68.0 - 1830 °F
Thermal Conductivity 5.00 W/m-K
@Temperature 20.0 °C
34.7 BTU-in/hr-ft²-°F
@Temperature 68.0 °F
 
Descriptive Properties
Colorblack (reduced form)
 gray

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
3M Techical Ceramics Ekasic® S Silicon Nitride
Goodfellow Gas Pressure Sintered Silicon Nitride Si3N4
Goodfellow High Thermal Conductivity Silicon Nitride
AISI Type F1 Tungsten High Speed Tool Steel
3M Techical Ceramics Ekatherm® Silicon Nitride

CMORF5085 / 200322

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.