MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Overview of materials for Silicone Foam
Categories: Polymer; Thermoset; Silicone; Silicone Foam

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Silicone Foam". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.104 - 1.64 g/cc0.00376 - 0.0592 lb/in³Average value: 0.410 g/cc Grade Count:43
Water Absorption 0.200 - 12.0 %0.200 - 12.0 %Average value: 4.15 % Grade Count:16
Viscosity 2.35 - 55000 cP2.35 - 55000 cPAverage value: 13300 cP Grade Count:10
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 3.00 - 62.03.00 - 62.0Average value: 23.1 Grade Count:8
Hardness, Shore OO 40.0 - 70.040.0 - 70.0Average value: 50.5 Grade Count:5
Tensile Strength, Ultimate 0.0552 - 2.80 MPa8.00 - 406 psiAverage value: 0.422 MPa Grade Count:21
Tensile Strength, Yield 0.172 - 1.24 MPa25.0 - 180 psiAverage value: 0.616 MPa Grade Count:7
Elongation at Break 49.0 - 300 %49.0 - 300 %Average value: 113 % Grade Count:30
Compressive Yield Strength 0.00800 - 0.170 MPa1.16 - 24.7 psiAverage value: 0.0659 MPa Grade Count:25
Compression Set 0.000 - 80.0 %0.000 - 80.0 %Average value: 12.8 % Grade Count:32
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.000100 - 1.00e+14 ohm-cm0.000100 - 1.00e+14 ohm-cmAverage value: 7.14e+13 ohm-cm Grade Count:7
Dielectric Constant 1.30 - 1.581.30 - 1.58Average value: 1.39 Grade Count:6
Dielectric Strength 3.50 - 7.48 kV/mm88.9 - 190 kV/inAverage value: 5.17 kV/mm Grade Count:13
Arc Resistance 90.0 - 123 sec90.0 - 123 secAverage value: 98.3 sec Grade Count:6
 
Thermal PropertiesMetricEnglishComments
CTE, linear 324 - 324 µm/m-°C
@Temperature 20.0 - 177 °C
180 - 180 µin/in-°F
@Temperature 68.0 - 350 °F
Average value: 324 µm/m-°C Grade Count:6
Specific Heat Capacity 1.26 J/g-°C0.300 BTU/lb-°FAverage value: 1.26 J/g-°C Grade Count:6
Thermal Conductivity 0.0600 - 0.163 W/m-K0.416 - 1.13 BTU-in/hr-ft²-°FAverage value: 0.0992 W/m-K Grade Count:14
Maximum Service Temperature, Air 150 - 280 °C302 - 536 °FAverage value: 219 °C Grade Count:18
Minimum Service Temperature, Air -70.0 - -20.0 °C-94.0 - -4.00 °FAverage value: -55.4 °C Grade Count:17
Brittleness Temperature -55.0 °C-67.0 °FAverage value: -55.0 °C Grade Count:5
Flammability, UL94 V-1 - V-0V-1 - V-0Grade Count:14
Flame Spread Index 11.5 - 25.011.5 - 25.0Average value: 22.6 Grade Count:10
Smoke Density 1.50 - 50.0 min1.50 - 50.0 minAverage value: 15.3 min Grade Count:15
Oxygen Index 34.0 - 44.0 %34.0 - 44.0 %Average value: 38.7 % Grade Count:6
 
Processing PropertiesMetricEnglishComments
Cure Time 10.0 - 60.0 min0.167 - 1.00 hourAverage value: 29.4 min Grade Count:7
 45.0 - 135 min
@Temperature 100 - 150 °C
0.750 - 2.25 hour
@Temperature 212 - 302 °F
Average value: 90.0 min Grade Count:2
Pot Life 0.500 - 240 min0.500 - 240 minAverage value: 50.0 min Grade Count:5

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Silicone Rubber
Overview of materials for Thermoset Polyurethane Foam, Unreinforced
Overview of materials for PVC, Foam Grade
Overview of materials for Silicone, RTV, Adhesive/Sealant Grade
Overview of materials for Liquid Silicone Rubber

O5203 / 78476

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.