MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Overview of materials for Nylon 6, 20% Glass Fiber Filled
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, 20% Glass Fiber Filled

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 20% Glass Fiber Filled".Specific grades with glass content between 15% and 24% are included. Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.14 - 1.67 g/cc0.0412 - 0.0603 lb/in³Average value: 1.25 g/cc Grade Count:582
 1.07 - 1.07 g/cc
@Temperature 270 - 270 °C
0.0387 - 0.0387 lb/in³
@Temperature 518 - 518 °F
Average value: 1.07 g/cc Grade Count:1
Filler Content 13.0 - 25.0 %13.0 - 25.0 %Average value: 17.4 % Grade Count:80
Water Absorption 0.150 - 9.50 %0.150 - 9.50 %Average value: 3.37 % Grade Count:231
Moisture Absorption at Equilibrium 0.170 - 8.00 %0.170 - 8.00 %Average value: 2.42 % Grade Count:183
 1.40 - 2.90 %
@Temperature 70.0 - 70.0 °C
1.40 - 2.90 %
@Temperature 158 - 158 °F
Average value: 2.37 % Grade Count:32
Water Absorption at Saturation 1.30 - 9.00 %1.30 - 9.00 %Average value: 7.40 % Grade Count:112
Additive Loading 15.0 - 20.0 %15.0 - 20.0 %Average value: 18.3 % Grade Count:3
Viscosity 2.90 - 3.00 cP2.90 - 3.00 cPAverage value: 2.94 cP Grade Count:5
 350 - 300000 cP
@Temperature 280 - 280 °C
350 - 300000 cP
@Temperature 536 - 536 °F
Average value: 150000 cP Grade Count:2
 350 - 300000 cP
@Shear Rate 1000 - 1000 1/s
350 - 300000 cP
@Shear Rate 1000 - 1000 1/s
Average value: 150000 cP Grade Count:2
Viscosity Test 125 - 150 cm³/g1.25 - 1.50 dl/gAverage value: 144 cm³/g Grade Count:14
Maximum Moisture Content 0.0200 - 0.2000.0200 - 0.200Average value: 0.140 Grade Count:17
 0.200 - 0.200
@Temperature 120 - 120 °C
0.200 - 0.200
@Temperature 248 - 248 °F
Average value: 0.200 Grade Count:3
 0.200 - 0.200
@Time 299 - 299 sec
0.200 - 0.200
@Time 0.0830 - 0.0830 hour
Average value: 0.200 Grade Count:3
Linear Mold Shrinkage 0.00100 - 0.0200 cm/cm0.00100 - 0.0200 in/inAverage value: 0.00523 cm/cm Grade Count:425
 0.00200 - 0.00800 cm/cm
@Temperature 80.0 - 80.0 °C
0.00200 - 0.00800 in/in
@Temperature 176 - 176 °F
Average value: 0.00520 cm/cm Grade Count:10
Linear Mold Shrinkage, Transverse 0.00100 - 0.0197 cm/cm0.00100 - 0.0197 in/inAverage value: 0.00812 cm/cm Grade Count:244
 0.00700 - 0.00900 cm/cm
@Temperature 80.0 - 80.0 °C
0.00700 - 0.00900 in/in
@Temperature 176 - 176 °F
Average value: 0.00800 cm/cm Grade Count:10
Melt Flow 2.00 - 100 g/10 min2.00 - 100 g/10 minAverage value: 28.2 g/10 min Grade Count:76
Spiral Flow 55.0 - 88.0 cm21.7 - 34.6 inAverage value: 81.9 cm Grade Count:14
Ash 13.0 - 20.0 %13.0 - 20.0 %Average value: 15.4 % Grade Count:12
 13.0 - 32.0 %
@Temperature 625 - 625 °C
13.0 - 32.0 %
@Temperature 1160 - 1160 °F
Average value: 20.2 % Grade Count:3
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 80.0 - 12180.0 - 121Average value: 104 Grade Count:21
Hardness, Rockwell R 90.0 - 12290.0 - 122Average value: 117 Grade Count:68
 10.0 - 12.0
@Temperature 80.0 - 80.0 °C
10.0 - 12.0
@Temperature 176 - 176 °F
Average value: 10.7 Grade Count:3
Hardness, Shore D 73.0 - 83.073.0 - 83.0Average value: 77.7 Grade Count:7
Ball Indentation Hardness 55.0 - 210 MPa7980 - 30500 psiAverage value: 145 MPa Grade Count:61
Tensile Strength, Ultimate 10.0 - 177 MPa1450 - 25600 psiAverage value: 101 MPa Grade Count:483
 10.0 - 190 MPa
@Temperature -40.0 - 150 °C
1450 - 27600 psi
@Temperature -40.0 - 302 °F
Average value: 76.1 MPa Grade Count:11
 50.0 - 60.0 MPa
@Temperature 80.0 - 80.0 °C
7250 - 8700 psi
@Temperature 176 - 176 °F
Average value: 76.1 MPa Grade Count:1
 50.0 - 60.0 MPa
@Strain 2.25 - 6.00 %
7250 - 8700 psi
@Strain 2.25 - 6.00 %
Average value: 76.1 MPa Grade Count:1
Tensile Strength, Yield 4.00 - 827 MPa580 - 120000 psiAverage value: 119 MPa Grade Count:113
 53.0 - 53.0 MPa
@Temperature 80.0 - 80.0 °C
7690 - 7690 psi
@Temperature 176 - 176 °F
Average value: 53.0 MPa Grade Count:1
Elongation at Break 1.00 - 28.0 %1.00 - 28.0 %Average value: 5.50 % Grade Count:522
 1.20 - 15.0 %
@Temperature -40.0 - 150 °C
1.20 - 15.0 %
@Temperature -40.0 - 302 °F
Average value: 4.74 % Grade Count:8
Elongation at Yield 2.00 - 100 %2.00 - 100 %Average value: 7.73 % Grade Count:39
 1.70 - 8.60 %
@Temperature 80.0 - 150 °C
1.70 - 8.60 %
@Temperature 176 - 302 °F
Average value: 3.76 % Grade Count:3
Modulus of Elasticity 0.0703 - 14.3 GPa10.2 - 2070 ksiAverage value: 5.16 GPa Grade Count:373
 1.70 - 6.50 GPa
@Temperature 60.0 - 150 °C
247 - 943 ksi
@Temperature 140 - 302 °F
Average value: 3.26 GPa Grade Count:2
Flexural Yield Strength 50.0 - 300 MPa7250 - 43500 psiAverage value: 156 MPa Grade Count:389
 45.0 - 275 MPa
@Temperature -40.0 - 90.0 °C
6530 - 39900 psi
@Temperature -40.0 - 194 °F
Average value: 126 MPa Grade Count:7
Flexural Modulus 0.650 - 40.3 GPa94.3 - 5850 ksiAverage value: 4.93 GPa Grade Count:426
 1.00 - 8.70 GPa
@Temperature -40.0 - 120 °C
145 - 1260 ksi
@Temperature -40.0 - 248 °F
Average value: 4.09 GPa Grade Count:9
Flexural Strain at Break 3.00 - 8.50 %3.00 - 8.50 %Average value: 6.02 % Grade Count:43
Compressive Yield Strength 65.0 - 155 MPa9430 - 22500 psiAverage value: 117 MPa Grade Count:10
 35.0 - 240 MPa
@Temperature -40.0 - 80.0 °C
5080 - 34800 psi
@Temperature -40.0 - 176 °F
Average value: 126 MPa Grade Count:3
Poissons Ratio 0.350 - 0.4400.350 - 0.440Average value: 0.360 Grade Count:13
Shear Modulus 2.30 - 2.60 GPa334 - 377 ksiAverage value: 2.45 GPa Grade Count:4
Shear Strength 65.0 - 115 MPa9430 - 16700 psiAverage value: 96.3 MPa Grade Count:3
Secant Modulus 0.750 - 7.00 GPa109 - 1020 ksiAverage value: 3.67 GPa Grade Count:5
 1.00 - 2.00 GPa
@Temperature 80.0 - 80.0 °C
145 - 290 ksi
@Temperature 176 - 176 °F
Average value: 1.50 GPa Grade Count:1
 1.00 - 2.00 GPa
@Strain 2.25 - 8.00 %
145 - 290 ksi
@Strain 2.25 - 8.00 %
Average value: 1.50 GPa Grade Count:1
Izod Impact, Notched 0.300 - 2.51 J/cm0.562 - 4.70 ft-lb/inAverage value: 0.881 J/cm Grade Count:153
 0.300 - 1.38814 J/cm
@Temperature -40.0 - -20.0 °C
0.562 - 2.60056 ft-lb/in
@Temperature -40.0 - -4.00 °F
Average value: 0.788 J/cm Grade Count:5
 0.588399 - 1.49492 J/cm
@Temperature -30.0 - -20.0 °C
1.10231 - 2.80060 ft-lb/in
@Temperature -22.0 - -4.00 °F
Average value: 0.788 J/cm Grade Count:5
 0.588399 - 1.49492 J/cm
@Thickness 3.17 - 6.40 mm
1.10231 - 2.80060 ft-lb/in
@Thickness 0.125 - 0.252 in
Average value: 0.788 J/cm Grade Count:5
Izod Impact, Unnotched 4.81 - 10.7 J/cm9.00 - 20.0 ft-lb/inAverage value: 6.78 J/cm Grade Count:15
Izod Impact, Notched (ISO) 4.00 - 40.0 kJ/m²1.90 - 19.0 ft-lb/in²Average value: 11.2 kJ/m² Grade Count:176
 3.00 - 13.0 kJ/m²
@Temperature -40.0 - -30.0 °C
1.43 - 6.19 ft-lb/in²
@Temperature -40.0 - -22.0 °F
Average value: 8.28 kJ/m² Grade Count:68
Izod Impact, Unnotched (ISO) 6.00 - 95.0 kJ/m²2.86 - 45.2 ft-lb/in²Average value: 54.0 kJ/m² Grade Count:58
 20.0 - 79.0 kJ/m²
@Temperature -40.0 - -30.0 °C
9.52 - 37.6 ft-lb/in²
@Temperature -40.0 - -22.0 °F
Average value: 46.5 kJ/m² Grade Count:44
Charpy Impact Unnotched 1.00 J/cm² - NB4.76 ft-lb/in² - NBAverage value: 6.39 J/cm² Grade Count:313
 0.680 J/cm² - NB
@Temperature -40.0 - -20.0 °C
3.24 ft-lb/in² - NB
@Temperature -40.0 - -4.00 °F
Average value: 4.91 J/cm² Grade Count:204
Charpy Impact, Notched 0.200 - 3.50 J/cm²0.952 - 16.7 ft-lb/in²Average value: 1.12 J/cm² Grade Count:359
 0.150 - 7.00 J/cm²
@Temperature -40.0 - -20.0 °C
0.714 - 33.3 ft-lb/in²
@Temperature -40.0 - -4.00 °F
Average value: 0.791 J/cm² Grade Count:199
Puncture Energy 2.00 - 32.0 J1.48 - 23.6 ft-lbAverage value: 8.43 J Grade Count:13
 1.50 - 4.80 J
@Temperature -30.0 - -30.0 °C
1.11 - 3.54 ft-lb
@Temperature -22.0 - -22.0 °F
Average value: 3.10 J Grade Count:11
Coefficient of Friction 0.1500.150Average value: 0.150 Grade Count:3
Tensile Creep Modulus, 1000 hours 2100 MPa305000 psiAverage value: 2100 MPa Grade Count:4
Taber Abrasion, mg/1000 Cycles 0.300 - 10.00.300 - 10.0Average value: 2.72 Grade Count:4
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 1000 - 1.00e+17 ohm-cm1000 - 1.00e+17 ohm-cmAverage value: 1.09e+15 ohm-cm Grade Count:245
Surface Resistance 100 - 1.00e+16 ohm100 - 1.00e+16 ohmAverage value: 2.40e+14 ohm Grade Count:151
Static Decay 2.00 sec2.00 secAverage value: 2.00 sec Grade Count:3
Dielectric Constant 2.50 - 19.02.50 - 19.0Average value: 5.51 Grade Count:102
Dielectric Strength 7.87 - 80.0 kV/mm200 - 2030 kV/inAverage value: 27.5 kV/mm Grade Count:157
Dissipation Factor 0.00550 - 0.3800.00550 - 0.380Average value: 0.0752 Grade Count:86
Dielectric Loss Index 0.0250 - 0.2400.0250 - 0.240Average value: 0.126 Grade Count:6
Arc Resistance 0.000 - 180 sec0.000 - 180 secAverage value: 117 sec Grade Count:13
Comparative Tracking Index 0.000 - 600 V0.000 - 600 VAverage value: 510 V Grade Count:170
 
Thermal PropertiesMetricEnglishComments
CTE, linear 16.0 - 57.6 µm/m-°C8.89 - 32.0 µin/in-°FAverage value: 33.8 µm/m-°C Grade Count:140
 15.0 - 24.0 µm/m-°C
@Temperature 55.0 - 160 °C
8.33 - 13.3 µin/in-°F
@Temperature 131 - 320 °F
Average value: 27.7 µm/m-°C Grade Count:3
 35.0 - 35.0 µm/m-°C
@Temperature 35.0 - 55.0 °C
19.4 - 19.4 µin/in-°F
@Temperature 95.0 - 131 °F
Average value: 27.7 µm/m-°C Grade Count:2
 35.0 - 35.0 µm/m-°C
@Thickness 2.00 - 2.00 mm
19.4 - 19.4 µin/in-°F
@Thickness 0.0787 - 0.0787 in
Average value: 27.7 µm/m-°C Grade Count:2
CTE, linear, Transverse to Flow 42.0 - 170 µm/m-°C23.3 - 94.4 µin/in-°FAverage value: 95.8 µm/m-°C Grade Count:79
 77.0 - 100 µm/m-°C
@Temperature 55.0 - 160 °C
42.8 - 55.6 µin/in-°F
@Temperature 131 - 320 °F
Average value: 89.0 µm/m-°C Grade Count:4
Specific Heat Capacity 1.60 - 1.70 J/g-°C0.382 - 0.406 BTU/lb-°FAverage value: 1.63 J/g-°C Grade Count:7
 2.47 - 2.47 J/g-°C
@Temperature 270 - 270 °C
0.590 - 0.590 BTU/lb-°F
@Temperature 518 - 518 °F
Average value: 2.47 J/g-°C Grade Count:1
Thermal Conductivity 0.310 - 0.432 W/m-K2.15 - 3.00 BTU-in/hr-ft²-°FAverage value: 0.348 W/m-K Grade Count:14
 0.190 - 0.200 W/m-K
@Temperature 270 - 270 °C
1.32 - 1.39 BTU-in/hr-ft²-°F
@Temperature 518 - 518 °F
Average value: 0.195 W/m-K Grade Count:2
Melting Point 210 - 315 °C410 - 599 °FAverage value: 222 °C Grade Count:352
Maximum Service Temperature, Air 65.0 - 200 °C149 - 392 °FAverage value: 140 °C Grade Count:57
Deflection Temperature at 0.46 MPa (66 psi) 150 - 303 °C302 - 577 °FAverage value: 211 °C Grade Count:252
Deflection Temperature at 1.8 MPa (264 psi) 58.0 - 280 °C136 - 536 °FAverage value: 194 °C Grade Count:416
Deflection Temperature at 8.0 MPa 50.0 - 120 °C122 - 248 °FAverage value: 61.8 °C Grade Count:28
Vicat Softening Point 177 - 308 °C351 - 586 °FAverage value: 206 °C Grade Count:116
Glass Transition Temp, Tg 10.0 - 135 °C50.0 - 275 °FAverage value: 66.4 °C Grade Count:6
UL RTI, Electrical 65.0 - 150 °C149 - 302 °FAverage value: 115 °C Grade Count:17
UL RTI, Mechanical with Impact 65.0 - 125 °C149 - 257 °FAverage value: 97.4 °C Grade Count:15
UL RTI, Mechanical without Impact 65.0 - 150 °C149 - 302 °FAverage value: 115 °C Grade Count:17
Flammability, UL94 HB - 5VAHB - 5VAGrade Count:308
Flame Spread 0.000 - 80.0 mm/min0.000 - 3.15 in/minAverage value: 30.9 mm/min Grade Count:9
Oxygen Index 21.0 - 34.0 %21.0 - 34.0 %Average value: 24.5 % Grade Count:31
Glow Wire Test 550 - 960 °C1020 - 1760 °FAverage value: 775 °C Grade Count:85
 
Processing PropertiesMetricEnglishComments
Processing Temperature 80.0 - 300 °C176 - 572 °FAverage value: 233 °C Grade Count:45
Nozzle Temperature 210 - 293 °C410 - 560 °FAverage value: 259 °C Grade Count:36
Melt Temperature 193 - 370 °C380 - 698 °FAverage value: 266 °C Grade Count:276
Mold Temperature 21.1 - 180 °C70.0 - 356 °FAverage value: 82.9 °C Grade Count:302
Drying Temperature 60.0 - 180 °C140 - 356 °FAverage value: 82.5 °C Grade Count:232
Moisture Content 0.0200 - 0.200 %0.0200 - 0.200 %Average value: 0.139 % Grade Count:124
Dew Point -17.8 °C0.000 °FAverage value: -17.8 °C Grade Count:7
Injection Pressure 3.45 - 172 MPa500 - 25000 psiAverage value: 79.1 MPa Grade Count:50

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Nylon 6, 10% Glass Fiber Filled
Overview of materials for Nylon 6, 30% Glass Fiber Filled
Overview of materials for Nylon 6, Unreinforced
Overview of materials for Nylon 6, 40% Glass Fiber Filled
Overview of materials for Nylon 6, 50% Glass Fiber Filled

O2412 / 77972

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.