MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Reade Advanced Materials Diatomaceous Earth (DE) (SiO2·nH2O)
Categories: Ceramic; Oxide; Silicon Oxide

Material Notes: Description: A naturally occurring mineral derived from microscopic in size fossilized remains of marine diatoms. It has high absorption, low bulk density and high brightness.
A silica source in the production of calcium silicates, insulation bricks and material in safes, fireproof filing cabinets, etc. Used in the paint, varnish, lacquer, and polish industries. Used as an insecticide in gardens and in swimming pools as a filtering agent.

Information provided by Reade Advanced Materials.

Key Words: SiO2*nH2O, Diatomaceous silica, diatomite, de, & kieselguhr
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 2.00 g/cc2.00 g/cc
Density 0.152 - 0.208 g/cc0.00550 - 0.00752 lb/in³Dry
Loss On Ignition 4.0 %4.0 %
pH 7.0 - 107.0 - 1010% slurry
 
Thermal PropertiesMetricEnglishComments
Melting Point 1715 °C3119 °F
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.461.46
 
Descriptive Properties
Coloroff-white to pink

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Thermal Ceramics Micro-Foil Type 475 Insulating Tape
Thermal Ceramics Micro-Foil Type E-Mat Insulating Tape
Sandvik Kanthal PAC-240A Wire insulations and coatings
China-Yixing Longly Refractories Microcrystal Wear-Resistant Alumina Grinding Media (Balls) and Lining Bricks
Chosun Refractories SSB-3 Bricks, Reaction Bonded SiC

CREADE007 / 1941

Elmet Technologies

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.