MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Schott AR-GLAS® Soda Lime Silicate Glass
Categories: Ceramic; Glass; Oxide; Silicon Oxide

Material Notes: Soda lime silicate glass, high dielectric constant, glass to metal seal, pharmaceutical primary packaging, general technical application

Information provided by SCHOTT AG.

Vendors: SCHOTT with its Business Unit Tubing offers tailor-made products & services worldwide from more than sixty special glass types for international growth markets such as industrial and environmental technology, electronics, display industry, architecture and design as well as pharmaceuticals. Contact us.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 2.50 g/cc
@Temperature 25.0 °C
0.0903 lb/in³
@Temperature 77.0 °F
 
Chemical PropertiesMetricEnglishComments
Acid Class, SR 11DIN 12116
Alkali Class, AR 22ISO 695
 
Thermal PropertiesMetricEnglishComments
CTE, linear 9.10 µm/m-°C
@Temperature 20.0 - 300 °C
5.06 µin/in-°F
@Temperature 68.0 - 572 °F
ISO 7991
Transformation Temperature, Tg 525 °C977 °F
Softening Point 720 °C1330 °FViscosity 107.6 dPa s
Working Point 1040 °C1900 °FViscosity 104 dPa s
Annealing Point 530 °C986 °FViscosity 1013 dPa s
 
Optical PropertiesMetricEnglishComments
Transmission, Visible 92 %
@Wavelength 400 - 800 nm,
Thickness 1.00 mm
92 %
@Wavelength 400 - 800 nm,
Thickness 0.0394 in
IR Transmittance  2.0 %
@Thickness 1.00 mm,
Wavelength 5000 nm
2.0 %
@Thickness 0.0394 in,
Wavelength 5000 nm
Cutoff
 20 %
@Thickness 1.00 mm,
Wavelength 4500 nm
20 %
@Thickness 0.0394 in,
Wavelength 4500 nm
 49 - 55 %
@Wavelength 2650 - 4100 nm,
Thickness 1.00 mm
49 - 55 %
@Wavelength 2650 - 4100 nm,
Thickness 0.0394 in
 90 - 92 %
@Wavelength 800 - 2500 nm,
Thickness 1.00 mm
90 - 92 %
@Wavelength 800 - 2500 nm,
Thickness 0.0394 in
 
Component Elements PropertiesMetricEnglishComments
Al2O3 4.0 %4.0 %
B2O3 1.0 %1.0 %
BaO 2.0 %2.0 %
CaO 5.0 %5.0 %
K2O 3.0 %3.0 %
MgO 3.0 %3.0 %
Na2O 13 %13 %
SiO2 69 %69 %
 
Descriptive Properties
Glasses in Laboratory ApparatusType IIASTM E 438
Hydrolytic ResistanceClass HGB 3ISO 719
 Type IIIPh. Eur.
 Type IIIUSP

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Borosilicate Glass
Schott Glass 8252 Alkaline Earth Aluminosilicate Glass
Overview of materials for Acrylic, Cast
Overview of materials for Low Alloy Steel
AISI 1045 Steel, as cold drawn, 16-22 mm (0.625-0.875 in) round

CSGS901 / 162006

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.