MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

PTS Trimid® N66-G13 13% Glass Fiber Reinforced Nylon 6/6  (discontinued **)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 10% Glass Fiber Filled

Material Notes: Information provided by Polymer Technology and Services, LLC (PTS).

Key Words: Polyamide 66; PA66
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.22 g/cc0.0441 lb/in³ASTM D792
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 100 MPa14500 psiASTM D638
Elongation at Break 2.0 %2.0 %ASTM D638
Flexural Modulus 4.65 GPa674 ksiASTM D790
Izod Impact, Notched 0.430 J/cm
@Thickness 3.17 mm
0.806 ft-lb/in
@Thickness 0.125 in
ASTM D256
 
Thermal PropertiesMetricEnglishComments
Melting Point 254 °C489 °FASTM D789
Deflection Temperature at 1.8 MPa (264 psi) 232 °C450 °FASTM D648
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 254 °C490 °F
Middle Barrel Temperature 268 °C515 °F
Front Barrel Temperature 285 °C545 °F
Nozzle Temperature 266 - 282 °C510 - 540 °F
Melt Temperature 271 - 293 °C520 - 560 °F
Mold Temperature 26.7 - 93.3 °C80.0 - 200 °F
Drying Temperature 71.1 °C160 °F
Dry Time 4 hour4 hour
Injection Pressure 68.9 MPa10000 psi
Back Pressure 0.0689 - 0.689 MPa10.0 - 100 psi
Screw Speed 30 - 60 rpm30 - 60 rpm

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Nylon 66, 10% Glass Fiber Filled
PTS Trimid® N66-G33 33% Glass Fiber Reinforced Nylon 6/6
PTS Trimid® N66-G13HL 13% Glass Fiber Reinforced Heat Stabilized, Lubed Nylon 6/6
Akro-Plastic Akromid® B3 GF 30 S1 (2091) PA66/6 Dry, 30% Glass Filled
PTS Trimid® N66-G33HL 33% Glass Fiber Reinforced Heat Stabilized, Lubed Nylon 6/6

PZ9PT45 / 21494

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.