MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Envalior Durethan® BKV 30 H2.0 EF 900116 Nylon 6, 30% Glass Fiber
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, 30% Glass Fiber Filled

Material Notes: PA 6, 30% glass fibers, good flowability (Easy Flow), good heat-ageing resistance

Former Lanxess product line is now with Envalior.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.35 g/cc0.0488 lb/in³ISO 1183
Melt Flow 101 g/10 min
@Load 5.00 kg,
Temperature 270 °C
101 g/10 min
@Load 11.0 lb,
Temperature 518 °F
Estimated using room temperature density; ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 100 MPa14500 psiConditioned; ISO 527-1/-2
 170 MPa24700 psiISO 527-1/-2
Elongation at Break 3.2 %3.2 %ISO 527-1/-2
 5.8 %5.8 %Conditioned; ISO 527-1/-2
Tensile Modulus 5.50 GPa798 ksiConditioned; ISO 527-1/-2
 9.00 GPa1310 ksiISO 527-1/-2
Charpy Impact Unnotched  5.50 J/cm²
@Temperature -30.0 °C
26.2 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eU
 5.50 J/cm²
@Temperature -30.0 °C
26.2 ft-lb/in²
@Temperature -22.0 °F
Conditioned; ISO 179/1eU
 6.00 J/cm²
@Temperature 23.0 °C
28.6 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eU
 8.00 J/cm²
@Temperature 23.0 °C
38.1 ft-lb/in²
@Temperature 73.4 °F
Conditioned; ISO 179/1eU
Charpy Impact, Notched  1.00 J/cm²
@Temperature 23.0 °C
4.76 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eA
 1.50 J/cm²
@Temperature 23.0 °C
7.14 ft-lb/in²
@Temperature 73.4 °F
Conditioned; ISO 179/1eA
Impact 803803Puncture maximum force (N); ISO 6603-2
 744
@Temperature -30.0 °C
744
@Temperature -22.0 °F
Puncture maximum force (N); ISO 6603-2
Puncture Energy 2.60 J1.92 ft-lbISO 6603-2
 2.60 J
@Temperature -30.0 °C
1.92 ft-lb
@Temperature -22.0 °F
ISO 6603-2
 2.60 J
@Temperature -30.0 °C
1.92 ft-lb
@Temperature -22.0 °F
Conditioned; ISO 6603-2
 
Electrical PropertiesMetricEnglishComments
Comparative Tracking Index 400 V400 VIEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 20.0 µm/m-°C11.1 µin/in-°FISO 11359-1/-2
CTE, linear, Transverse to Flow 100 µm/m-°C55.6 µin/in-°FISO 11359-1/-2
Melting Point 220 °C428 °F10°C/min; ISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi) 220 °C428 °FISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 210 °C410 °FISO 75-1/-2
Deflection Temperature at 8.0 MPa 150 °C302 °FISO 75-1/-2
 
Descriptive Properties
AdditivesRelease agent
FormPellets
ISO Short NameISO1874-PA6, MHR, 10-090, GF30
ProcessingInjection molding
RegionAsia Pacific
 Europe
 Near East/Africa
 North America
 South and Central America

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Envalior Durethan® BKV 30 H2.0 EF 000000 Nylon 6, Glass Fiber Reinforced
Envalior Durethan® BKV 130 H3.0 101006 Copolyamide, 30% Glass Fiber
Envalior Akulon® Ultraflow K-FG6 PA6-GF30, Conditioned, 30% Glass Filled, High Flow

PLANX0769 / 98984

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.