MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Ethydco Advancene™ EE-3914-AAH Medium Density Polyethylene Resin
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Film Grade

Material Notes: Blown film. This high molecular weight hexene copolymer provides: excellent overall balance of processability, toughness, and strength, good impact strength and tear properties. Applications: general purpose this film, trash bags, merchant bags, blending partner, produce bags, shopping bags.

Information provided by ETHYDCO.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.939 g/cc0.0339 lb/in³ASTM D792
Melt Index of Compound 14 g/10 min
@Load 2.16 kg,
Temperature 190 °C
14 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238, ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Film Tensile Strength at Yield, MD 21.0 MPa3050 psi50 mm/min; ASTM D882
Film Tensile Strength at Yield, TD 23.0 MPa3340 psi50 mm/min; ASTM D882
Film Elongation at Break, MD 500 %500 %50mm/min; ASTM D882
Film Elongation at Break, TD 660 %660 %50mm/min; ASTM D882
Flexural Modulus 0.760 GPa110 ksitangent; ASTM D790B
Elmendorf Tear Strength MD 30 g30 gASTM 1922
Elmendorf Tear Strength TD 350 g350 gASTM 1922
Dart Drop Test 165 g0.364 lbASTM 1709A, ISO 7765
Film Tensile Strength at Break, MD 35.0 MPa5080 psiASTM D882
Film Tensile Strength at Break, TD 27.0 MPa3920 psiASTM D882
 
Thermal PropertiesMetricEnglishComments
Brittleness Temperature <= -75.0 °C<= -103 °FASTM D746
 
Descriptive Properties
Spencer Impact Strength (J)0.35ASTM D3420

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Borealis Borstar® FB3450 HDPE for Film Extrusion
Borealis Bormed™ HE2581-PH HDPE for Healthcare Applications
Chevron Phillips Marlex® HMN TR-935/935G Polyethylene; MDPE
Polimeros Mexicanos Rotolene® 93050 Medium Density Polyethylene
Dow DFDC-7525 NT High Density Polyethylene Resin

PETHYD907 / 200053

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.