MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

LATI Lasulf PSU
Categories: Polymer; Thermoplastic; Polysulfone (PSU)

Material Notes: Polysulfone (PSU). Unfilled. Low smoke density and low toxicity index. Very high dimensional stability.

Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North America

Information provided by Lati Industria Termoplastici S.p.A.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.23 g/cc0.0444 lb/in³
Linear Mold Shrinkage, Flow 0.0060 - 0.0090 cm/cm0.0060 - 0.0090 in/in
Linear Mold Shrinkage, Transverse 0.0065 - 0.0095 cm/cm0.0065 - 0.0095 in/in
 
Mechanical PropertiesMetricEnglishComments
Elongation at Break  >= 100 %
@Temperature 23.0 °C
>= 100 %
@Temperature 73.4 °F
 >= 100 %
@Temperature 60.0 °C
>= 100 %
@Temperature 140 °F
 >= 100 %
@Temperature 90.0 °C
>= 100 %
@Temperature 194 °F
 >= 100 %
@Temperature 120 °C
>= 100 %
@Temperature 248 °F
 >= 100 %
@Temperature 150 °C
>= 100 %
@Temperature 302 °F
Elongation at Yield  2.8 %
@Temperature 150 °C
2.8 %
@Temperature 302 °F
 3.5 %
@Temperature 120 °C
3.5 %
@Temperature 248 °F
 4.0 %
@Temperature 90.0 °C
4.0 %
@Temperature 194 °F
 4.5 %
@Temperature 60.0 °C
4.5 %
@Temperature 140 °F
 5.5 %
@Temperature 23.0 °C
5.5 %
@Temperature 73.4 °F
Tensile Modulus  1.90 GPa
@Temperature 150 °C
276 ksi
@Temperature 302 °F
 2.00 GPa
@Temperature 120 °C
290 ksi
@Temperature 248 °F
 2.20 GPa
@Temperature 90.0 °C
319 ksi
@Temperature 194 °F
 2.30 GPa
@Temperature 60.0 °C
334 ksi
@Temperature 140 °F
 2.50 GPa
@Temperature 23.0 °C
363 ksi
@Temperature 73.4 °F
Charpy Impact Unnotched  NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
 NB
@Temperature -20.0 °C
NB
@Temperature -4.00 °F
Charpy Impact, Notched  0.150 J/cm²
@Temperature -20.0 °C
0.714 ft-lb/in²
@Temperature -4.00 °F
 0.500 J/cm²
@Temperature 23.0 °C
2.38 ft-lb/in²
@Temperature 73.4 °F
 
Electrical PropertiesMetricEnglishComments
Comparative Tracking Index 150 V150 VA solution
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 150 °C302 °F
Deflection Temperature at 0.46 MPa (66 psi) 180 °C356 °F
Deflection Temperature at 1.8 MPa (264 psi) 165 °C329 °F
Vicat Softening Point 175 °C
@Load 5.00 kg
347 °F
@Load 11.0 lb
Flammability, UL94  HB
@Thickness 1.50 mm
HB
@Thickness 0.0591 in
 V-1
@Thickness 3.00 mm
V-1
@Thickness 0.118 in
Oxygen Index 30 %30 %
Glow Wire Test  960 °C
@Thickness 1.00 mm
1760 °F
@Thickness 0.0394 in
GWFI/GWT
 960 °C
@Thickness 2.00 mm
1760 °F
@Thickness 0.0787 in
GWFI/GWT
 
Processing PropertiesMetricEnglishComments
Melt Temperature 290 - 320 °C554 - 608 °F
Mold Temperature 110 - 130 °C230 - 266 °F
Drying Temperature 110 - 130 °C
@Time 10800 sec
230 - 266 °F
@Time 3.00 hour
 
Descriptive Properties
ISO Shrinkage - Pressure60 MPa

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Gharda Chemicals GAFONE™-S 1400 PSU, High Thermal Stability
Evonik Trogamid® CX7323 Transparent Nylon
BASF Ultrason® S 2010 PSU
Ensinger NORYL® Polyphenylene oxide (PPO)
LATI Lasulf G/30 PSU, 30% Glass Fiber Reinforced

PLATH9671 / 177367

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.