MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Pyrotek PT-10 Graphite
Categories: Carbon; Graphite

Material Notes: PT-10 Graphite offers the highest resistance to oxidation available. Its unique composition gives it the most durable, long lasting, oxidation resistant properties available from treated graphite.

Applications

  • Degassing shafts
  • Stators
  • Pump shafts and posts

Advantages

  • High strength
  • Up to 2-3 times the life, depending on the application

Information provided by Pyrotek.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.85 g/cc0.0668 lb/in³
Porosity 6.0 %6.0 %
 
Mechanical PropertiesMetricEnglishComments
Flexural Strength 26.0 MPa3770 psiacross grain
 28.0 MPa4060 psiwith grain
Compressive Strength 41.0 MPa5950 psiacross grain
 48.0 MPa6960 psiwith grain
 
Thermal PropertiesMetricEnglishComments
CTE, linear  3.40 µm/m-°C
@Temperature 20.0 °C
1.89 µin/in-°F
@Temperature 68.0 °F
with grain
 4.50 µm/m-°C
@Temperature 20.0 °C
2.50 µin/in-°F
@Temperature 68.0 °F
across grain

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Graphite, Carbon, C
Pyrotek PTB 2200 Structural Board
NeoGraf eGRAF® HITHERM™ HT-1220 Graphite
Pyrotek PROSILY G-10R Graphite Lubricant/Coating
Pyrotek PROSILY G-11R Graphite Lubricant/Coating

CPYRO156 / 1876

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.