Color - Black, Base - Graphite, Carrier - Resin Applications - Mold coating
- Extrusion die
- Dry film lubricator
Advantages - Resistant to high temperature
- Good thermal conductivity
- Low coefficient of expansion
- Chemically inert
Information provided by Pyrotek. |