MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Overview of materials for Polypropylene with 30% Talc Filler
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene with 30% Talc Filler

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 30% Talc Filler". Specific grades with primary filler content between 25% and 34% are included. Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.05 - 1.48 g/cc0.0379 - 0.0535 lb/in³Average value: 1.13 g/cc Grade Count:226
Filler Content 25.0 - 32.0 %25.0 - 32.0 %Average value: 29.2 % Grade Count:81
Water Absorption 0.000 - 0.0500 %0.000 - 0.0500 %Average value: 0.0256 % Grade Count:16
Linear Mold Shrinkage 0.00500 - 0.0212 cm/cm0.00500 - 0.0212 in/inAverage value: 0.0111 cm/cm Grade Count:133
Linear Mold Shrinkage, Transverse 0.00700 - 0.0211 cm/cm0.00700 - 0.0211 in/inAverage value: 0.0125 cm/cm Grade Count:52
Melt Flow 0.500 - 230 g/10 min0.500 - 230 g/10 minAverage value: 13.9 g/10 min Grade Count:212
Ash 25.0 - 32.0 %25.0 - 32.0 %Average value: 29.8 % Grade Count:18
 28.0 - 30.0 %
@Temperature 700 - 900 °C
28.0 - 30.0 %
@Temperature 1290 - 1650 °F
Average value: 29.0 % Grade Count:2
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 49.0 - 10049.0 - 100Average value: 67.0 Grade Count:4
Hardness, Rockwell R 45.0 - 10045.0 - 100Average value: 79.2 Grade Count:25
Hardness, Shore D 64.0 - 82.064.0 - 82.0Average value: 72.2 Grade Count:18
Ball Indentation Hardness 44.0 - 58.0 MPa6380 - 8410 psiAverage value: 51.7 MPa Grade Count:3
Tensile Strength, Ultimate 13.0 - 37.3 MPa1890 - 5400 psiAverage value: 26.0 MPa Grade Count:114
Tensile Strength, Yield 2.48 - 72.0 MPa360 - 10400 psiAverage value: 25.3 MPa Grade Count:118
Elongation at Break 3.00 - 250 %3.00 - 250 %Average value: 24.9 % Grade Count:113
 >= 100 %
@Temperature 60.0 - 90.0 °C
>= 100 %
@Temperature 140 - 194 °F
Average value: 100 % Grade Count:1
Elongation at Yield 2.70 - 80.0 %2.70 - 80.0 %Average value: 7.90 % Grade Count:73
 5.00 - 6.00 %
@Temperature 60.0 - 90.0 °C
5.00 - 6.00 %
@Temperature 140 - 194 °F
Average value: 5.50 % Grade Count:1
Modulus of Elasticity 1.50 - 4.00 GPa218 - 580 ksiAverage value: 2.66 GPa Grade Count:55
 0.500 - 1.10 GPa
@Temperature 60.0 - 90.0 °C
72.5 - 160 ksi
@Temperature 140 - 194 °F
Average value: 0.800 GPa Grade Count:1
Flexural Yield Strength 20.0 - 105 MPa2900 - 15200 psiAverage value: 46.2 MPa Grade Count:97
Flexural Modulus 1.40 - 19.7 GPa203 - 2850 ksiAverage value: 2.60 GPa Grade Count:224
 2.60 - 3.70 GPa
@Temperature -20.0 - -20.0 °C
377 - 537 ksi
@Temperature -4.00 - -4.00 °F
Average value: 3.15 GPa Grade Count:2
Izod Impact, Notched 0.149 - 2.67 J/cm0.280 - 5.00 ft-lb/inAverage value: 0.531 J/cm Grade Count:82
 0.300 - 1.00 J/cm
@Temperature -40.0 - 0.000 °C
0.562 - 1.87 ft-lb/in
@Temperature -40.0 - 32.0 °F
Average value: 0.512 J/cm Grade Count:3
Izod Impact, Unnotched 0.470 - 5340 J/cm0.881 - 10000 ft-lb/inAverage value: 3.31 J/cm Grade Count:16
Izod Impact, Notched (ISO) 2.00 - 40.0 kJ/m²0.952 - 19.0 ft-lb/in²Average value: 10.2 kJ/m² Grade Count:53
 1.90 - 3.50 kJ/m²
@Temperature -40.0 - -30.0 °C
0.904 - 1.67 ft-lb/in²
@Temperature -40.0 - -22.0 °F
Average value: 2.62 kJ/m² Grade Count:13
Charpy Impact Unnotched 2.50 J/cm² - NB11.9 ft-lb/in² - NBAverage value: 4.93 J/cm² Grade Count:58
 1.10 J/cm² - NB
@Temperature -40.0 - 0.000 °C
5.24 ft-lb/in² - NB
@Temperature -40.0 - 32.0 °F
Average value: 2.64 J/cm² Grade Count:30
Charpy Impact, Notched 0.200 - 3.50 J/cm²0.952 - 16.7 ft-lb/in²Average value: 0.978 J/cm² Grade Count:98
 0.0300 - 0.600 J/cm²
@Temperature -40.0 - -20.0 °C
0.143 - 2.86 ft-lb/in²
@Temperature -40.0 - -4.00 °F
Average value: 0.277 J/cm² Grade Count:63
Gardner Impact 0.565 - 36.2 J0.417 - 26.7 ft-lbAverage value: 5.23 J Grade Count:25
 5.53626 - 5.53626 J
@Temperature -30.0 - -30.0 °C
4.08334 - 4.08334 ft-lb
@Temperature -22.0 - -22.0 °F
Average value: 6.89 J Grade Count:1
 7.23 - 7.23 J
@Temperature -23.0 - -23.0 °C
5.33 - 5.33 ft-lb
@Temperature -9.40 - -9.40 °F
Average value: 6.89 J Grade Count:2
 7.23 - 7.23 J
@Thickness 3.18 - 3.18 mm
5.33 - 5.33 ft-lb
@Thickness 0.125 - 0.125 in
Average value: 6.89 J Grade Count:2
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 1.00e+16 ohm-cm1.00e+16 ohm-cmAverage value: 1.00e+16 ohm-cm Grade Count:3
Surface Resistance 1.00e+13 ohm1.00e+13 ohmAverage value: 1.00e+13 ohm Grade Count:5
Dielectric Constant 2.40 - 2.602.40 - 2.60Average value: 2.50 Grade Count:4
Dielectric Strength 19.7 - 24.0 kV/mm500 - 610 kV/inAverage value: 22.3 kV/mm Grade Count:5
Comparative Tracking Index 600 V600 VAverage value: 600 V Grade Count:6
 
Thermal PropertiesMetricEnglishComments
CTE, linear 48.6 - 100 µm/m-°C27.0 - 55.6 µin/in-°FAverage value: 75.2 µm/m-°C Grade Count:14
Melting Point 150 - 182 °C302 - 360 °FAverage value: 159 °C Grade Count:21
Deflection Temperature at 0.46 MPa (66 psi) 54.0 - 144 °C129 - 291 °FAverage value: 118 °C Grade Count:128
Deflection Temperature at 1.8 MPa (264 psi) 50.0 - 143 °C122 - 289 °FAverage value: 72.0 °C Grade Count:155
Vicat Softening Point 45.0 - 192 °C113 - 378 °FAverage value: 104 °C Grade Count:119
Flammability, UL94 HB - V-0HB - V-0Grade Count:89
Oxygen Index 21.0 %21.0 %Average value: 21.0 % Grade Count:6
Glow Wire Test 550 - 750 °C1020 - 1380 °FAverage value: 726 °C Grade Count:33
 
Processing PropertiesMetricEnglishComments
Processing Temperature 193 - 227 °C380 - 440 °FAverage value: 210 °C Grade Count:3
Nozzle Temperature 200 - 260 °C392 - 500 °FAverage value: 222 °C Grade Count:20
Adapter Temperature 200 - 210 °C392 - 410 °FAverage value: 205 °C Grade Count:6
Die Temperature 200 - 210 °C392 - 410 °FAverage value: 205 °C Grade Count:6
Melt Temperature 170 - 279 °C338 - 534 °FAverage value: 219 °C Grade Count:99
Mold Temperature 10.0 - 90.0 °C50.0 - 194 °FAverage value: 48.6 °C Grade Count:94
Drying Temperature 51.7 - 220 °C125 - 428 °FAverage value: 80.2 °C Grade Count:81
Moisture Content 0.0500 - 0.200 %0.0500 - 0.200 %Average value: 0.0688 % Grade Count:20
Injection Pressure 2.76 - 130 MPa400 - 18900 psiAverage value: 68.9 MPa Grade Count:63

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Polypropylene with 20% Talc Filler
Overview of materials for Polypropylene with 40% Talc Filler
Overview of materials for Polypropylene with 10% Talc Filler
Overview of materials for Polypropylene with 30% Glass Fiber Filler
Overview of materials for Polypropylene, Molded

O4763 / 78400

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.