MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Polycasa SAN
Categories: Polymer; Thermoplastic; SAN Polymer

Material Notes: QUINN SAN sheets are characterized by good optical properties and a brilliant surface. The QUINN SAN range contains sheets that are easy to handle, to vacuum form, and show a very good dimensional stability. Typical for QUINN SAN sheets are their very good chemical resistance: they are resistant to most fats, dilute acid solutions, oils and common bleaching agents, as well as some solvents and weak alkaline solutions. The sheets can be used in- and outdoor (in UVP-version) and are resistant to temperature fluctuations. QUINN SAN products can be used in contact with foodstuffs. QUINN SAN material also combines the following excellent properties: High softening point, low water absorption, and high stiffness.
  • Industrial (door) glazing
  • Covers for foodstuffs
  • Covers for office equipment
  • Screen printing
  • Advertising signs
  • Fittings for shops and exhibitions
  • Displays Flat or curved shower screens
  • Greenhouse glazing
  • Room dividers

Quinn Manufacturing Group rebranded its Plastics Division as Polycasa in 2013.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.08 g/cc0.0390 lb/in³ISO 1183
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 8383ISO 2039-2
Tensile Strength at Break 60.0 MPa8700 psiISO 527-2
Elongation at Break 1.8 %1.8 %ISO 527-2
Tensile Modulus 3.90 GPa566 ksiISO 527-2
Flexural Strength 105 MPa15200 psiISO 178
Flexural Modulus 3.75 GPa544 ksiISO 178
Izod Impact, Notched (ISO) 1.30 kJ/m²0.619 ft-lb/in²ISO 180
Charpy Impact Unnotched 1.30 J/cm²6.19 ft-lb/in²ISO 179-1
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+14 ohm-cm1.00e+14 ohm-cmIEC 6093
Surface Resistance >= 1.00e+14 ohm>= 1.00e+14 ohmIEC 6093
 
Thermal PropertiesMetricEnglishComments
CTE, linear 50.0 - 70.0 µm/m-°C
@Temperature 20.0 °C
27.8 - 38.9 µin/in-°F
@Temperature 68.0 °F
DIN 53752
Specific Heat Capacity 1.38 J/g-°C0.330 BTU/lb-°FASTM D2766
Thermal Conductivity 0.170 W/m-K1.18 BTU-in/hr-ft²-°FDIN 52612
Maximum Service Temperature, Air 85.0 °C185 °F
Deflection Temperature at 0.46 MPa (66 psi) 101 °C214 °FISO 75
Deflection Temperature at 1.8 MPa (264 psi) 98.0 °C208 °FISO 75
Vicat Softening Point 106 °C223 °FISO 306
Decomposition Temperature >= 280 °C>= 536 °F
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.571.57ISO 489
Transmission, Visible 86 %86 %DIN 5036-3
 
Processing PropertiesMetricEnglishComments
Processing Temperature 165 - 190 °C329 - 374 °FSheet Forming

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Covestro Makroblend® UT-250 Polycarbonate + Polyester Blend
Covestro Makroblend® UT250 HR PC+PET
Covestro Makroblend® UT-400 Polycarbonate + Polyester Blend
Lucite International Elvacite® 2669 Acrylic Resin
LG Chemical 95HC SAN Resin

PSF023B / 66592

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.