MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Lucite International Elvacite® 2669 Acrylic Resin
Categories: Polymer; Thermoplastic; Acrylic (PMMA)

Material Notes: Elvacite® 2669, the first in this series, is a solid acrylic bead copolymer which can be dissolved in slightly alkaline aqueous systems. This distinct capability makes the product particularly suitable for end-uses where solvent emissions must be minimized or where the substrate may be sensitive to organic solvents. Clear, hard, abrasion resistant films and coatings may be obtained due to the polymethyl methacrylate backbone of this specially modified resin. These films show good adhesion to numerous substrates such as metal and plastic.

The water-soluble characteristics of this polymer allow for its use in areas where temporary protection is desirable. Dilute ammoniated solutions may be used to remove the film. If a more permanent coating is required, formulations with zinc oxide may be prepared to enhance durability and improve water resistance. Elvacite® 2669 further exhibits good solubility in many ketones and esters as well as glycol ethers. Plasticizers such as butyl benzyl phthalate may be added to enhance flexibility and flow properties.

Information provided by Lucite International

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.20 g/cc1.20 g/cc
Density 1.10 g/cc0.0398 lb/in³ASTM D-1475
Viscosity Measurement 0.320.32Inherent viscosity
Molecular Weight 60000 g/mol60000 g/mol
 
Chemical PropertiesMetricEnglishComments
Total Acid Number 124124
 
Thermal PropertiesMetricEnglishComments
Glass Transition Temp, Tg 70.0 °C158 °F
 
Descriptive Properties
Gardner-Holdt ViscosityZ-6

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Covestro Makroblend® UT-400 Polycarbonate + Polyester Blend
Covestro Makroblend® UT-250 Polycarbonate + Polyester Blend
Covestro Arcol® PPG-425 Polypropylene Glycol
Polycasa SAN
Eastman Vanceva® Polyvinyl Butyral Interlayer

PLUCIT9468 / 150182

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.