MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Mueller Ecostream™ C36500 Uninhibited Leaded Muntz Metal
Categories: Metal; Nonferrous Metal; Copper Alloy; Brass

Material Notes: Mueller Brass Company’s C36500 alloy provides a viable alternative to those manufacturers who are manufacturing products and components that require compliance with the recently approved “Reduction of Lead in Drinking Water Act.” The legislation re-defines the term “lead free” to mean “… no more that a weighted average of 0.25% lead when used with respect to the wetted surfaces of pipes, plumbing fittings and fixtures.” With this in mind, Mueller Brass Company’s C36500 alloy provides a lower percentage lead alloy (versus conventional free cutting and forging alloys) that aids in the compliance to this legislation while maintaining machinability ratings near that of conventional free cutting brass.
No Silicon • No Bismuth • No Segregation
In addition to machinability ratings near that of free cutting brass, C36500 also possesses the virtues and merits of Mueller Brass Company’s other EcoStream™ Lead Free and Low Lead alloys. Since no contaminating additives like bismuth or silicon are used in the production of this alloy, C36500 is completely recyclable with conventional brass alloys still widely being used for non-potable plumbing and industrial applications.

Advantanges:

  • Excellent machinability
  • Excellent forgeability
  • Excellent Brazing and Plating
  • Excellent ability to Thread Roll
  • Completely recyclable

Applications:

  • Screw machine parts requiring lower lead content
  • Potable water components, fixtures, and applications
  • Forged components in LEAD FREE compliant products

Information Provided by Mueller Industries Inc.

Key Words: ASTM B124, UNS C36500
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.41 g/cc0.304 lb/in³Based on UNS number
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell B 70 - 7570 - 75
Tensile Strength at Break 414 MPa60000 psi
Tensile Strength, Yield 276 MPa40000 psi
Elongation at Break 30 %30 %
 
Component Elements PropertiesMetricEnglishComments
Copper, Cu 58 - 61 %58 - 61 %
Iron, Fe <= 0.15 %<= 0.15 %
Lead, Pb 0.25 - 0.70 %0.25 - 0.70 %
Tin, Sn <= 0.25 %<= 0.25 %
Zinc, Zn 37.9 - 41.75 %37.9 - 41.75 %Remainder

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Syensqo (Solvay Specialty Polymers) Amodel® FC-1150 Polyphthalamide (PPA), 50% Glass Fiber
ExxonMobil Santoprene® 141-55W185 Thermoplastic Elastomer
CMT Materials HYTAC® FLX Good Durability, Easily Machined & Polished Copolymer Syntactic
Borealis RA7050 Polypropylene-Random-Copolymer for Pressure Pipe Systems
Borealis RA130E-1498 Polypropylene Random Copolymer

NMUEL905 / 97693

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.