MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

USP Class VI Adhesives
USP Class VI Approved Adhesives for Medical Device Applications
Master Bond’s biocompatible adhesives are designed to meet the needs of medical device manufacturers. Compounds withstand various types of sterilization methods.

Eastman Eastar MN058 Copolyester
Categories: Polymer; Thermoplastic; Polyester, TP

Material Notes: Product Description: Meets ISO 10993 and/or USP Class VI biocompatibility requirements. Eastar™ Copolyester MN058 is a medical grade base with brilliantly cl ear polymers that have excellent impact strength, chemical resistance, dimensional stability, and low shrinkage rates. It has a relatively high flex modulus and yield strength. This product has high flow characteristics. It does not contain a mold release or ultraviolet stabilizer. This product has been GREENGUARD INDOOR AIR QUALITY CERTIFIED

Applications/Uses:

  • Drug Delivery
  • Labware
  • Medical
Key Attributes:
  • Chemical resistance to most medical solvents including lipids and IPA
  • Gamma and E-beam color stability

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.33 g/cc1.33 g/ccASTM D792
Water Absorption 0.19 %0.19 %24h Immersion; ASTM D570
Linear Mold Shrinkage 0.0020 cm/cm0.0020 in/inASTM D955
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 111111ASTM D785
Tensile Strength at Break 24.0 MPa3480 psiASTM D638
Tensile Strength, Yield 58.0 MPa8410 psiASTM D638
Elongation at Break 90 %90 %ASTM D638
Elongation at Yield 4.0 %4.0 %ASTM D638
Flexural Yield Strength 78.0 MPa11300 psiASTM D790
Flexural Modulus 2.40 GPa348 ksiASTM D790
Izod Impact, Notched  0.330 J/cm
@Temperature -40.0 °C
0.618 ft-lb/in
@Temperature -40.0 °F
ASTM D256
 0.560 J/cm
@Temperature 23.0 °C
1.05 ft-lb/in
@Temperature 73.4 °F
ASTM D256
Izod Impact, Unnotched NBNBASTM D4812
 24.46 J/cm
@Temperature -40.0 °C
45.82 ft-lb/in
@Temperature -40.0 °F
ASTM D4812
Puncture Energy 32.0 J23.6 ft-lbPuncture Resistance @Max Load, 23°C; ASTM D3763
 38.0 J
@Temperature -40.0 °C
28.0 ft-lb
@Temperature -40.0 °F
Puncture Resistance at Max Load; ASTM D3763
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 69.0 °C156 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 63.0 °C145 °FASTM D648
Vicat Softening Point 80.0 °C176 °F1kg load; ASTM D1525
 
Optical PropertiesMetricEnglishComments
Haze <= 1.0 %<= 1.0 %ASTM D1003
Transmission, Visible 82 %82 %Total Transmittance; ASTM D1003
 
Processing PropertiesMetricEnglishComments
Melt Temperature 277 - 293 °C531 - 559 °F
Mold Temperature 16.0 - 32.0 °C60.8 - 89.6 °F
Drying Temperature 160 °C320 °F
Dry Time 4 - 6 hour4 - 6 hour
 
Compliance PropertiesMetricEnglishComments
USP Class VI YesYes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
INEOS Styrolution PS 124 N/L GPPS
Delrin Delrin® 127UV NC010 POM
Tabriz HD 6070EA High Density Polyethylene Copolymer
Eastman Tritan™ MP100 Copolyester
INEOS Styrolution Zylar® 650 MBS

PE9052 / 35108

USP Class VI adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.