MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Tabriz HD 6070EA High Density Polyethylene Copolymer
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Injection Molded

Material Notes: HD6070EA is high density polyethylene copolymer containing butene-1(C4) as comonomer with good impact strength, easy processing, high warpage resistance, high rigidity medium content of light stabilizer additive. It is suitable for general purpose injection molding items. HD6070EA has the following characteristics: This grade has food contact approval.

Information provided by Tabriz Petrochemical Company.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.960 g/cc0.0347 lb/in³ASTM D1505
Brightness 60.0 %60.0 %Whiteness Index; ASTM E313
Melt Flow 7.0 g/10 min
@Load 2.16 kg
7.0 g/10 min
@Load 4.76 lb
ASTM D-1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 26.0 MPa3770 psiASTM D638
Elongation at Break 900 %900 %ASTM D638
Charpy Impact, Notched 0.500 J/cm²2.38 ft-lb/in²ASTM D6110
 
Thermal PropertiesMetricEnglishComments
Vicat Softening Point 120 °C248 °FASTM D1525
 
Optical PropertiesMetricEnglishComments
Yellow Index -1.00 %-1.00 %ASTM E313
 
Descriptive Properties
Contamination (No.)5BP137

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Eastman Eastar MN058 Copolyester
INEOS Styrolution PS 124 N/L GPPS
Braskem Flexus® 7200 Cast Film Extrusion Polyethylene
Amco PRIMATOP HDPE 002955 Phillips Process Hexene Copolymer
NOVA Chemicals Sclair® 17A Butene HDPE Film Resin

PTABRZ902 / 198214

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.