MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

NOVA Chemicals Sclair® 17A Butene HDPE Film Resin
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Film Grade

Material Notes: 17A complies with the U.S. FDA specifications for olefin polymers and may thus be used in the United States as an article or component of an article intended for use in contact with food, without temperature or food-type restrictions, subject to technical suitability.

NOVA Chemicals' polyethylene resins are chemically and biologically inert.

Features: Low gel, Good processability

Additives: Process stabilizer

Applications: Co-extrusions, Blending

Properties measured from film produced on a laboratory extruder with a 4 inch die, 35 mil die gap, and a BUR of 2.5:1

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.950 g/cc0.0343 lb/in³ASTM D 792
Oxygen Transmission Rate 1920 cc/m²/day124 cc/100 in²/day0% RH; ASTM D 1434
Thickness 38.0 microns1.50 mil
Melt Flow 0.45 g/10 min
@Load 2.16 kg,
Temperature 190 °C
0.45 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D 1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 6767ASTM D 2240
Film Tensile Strength at Yield, MD 22.0 MPa3190 psiASTM D 882
Film Tensile Strength at Yield, TD 20.0 MPa2900 psiASTM D 882
Film Elongation at Break, MD 650 %650 %ASTM D 882
Film Elongation at Break, TD 750 %750 %ASTM D 882
Coefficient of Friction 0.240.24ASTM D 1894
Elmendorf Tear Strength MD 22 g22 gASTM D 1922
Elmendorf Tear Strength TD 875 g875 gASTM D 1922
Elmendorf Tear Strength, MD 0.600 g/micron15.2 g/milASTM D 1922
Elmendorf Tear Strength, TD 23.0 g/micron584 g/mil
Dart Drop Test 40.0 g0.0882 lb1.1; ASTM D 1709/A
Film Tensile Strength at Break, MD 45.0 MPa6530 psiASTM D 882
Film Tensile Strength at Break, TD 20.0 MPa2900 psiASTM D 882
1% Secant Modulus, MD 630 MPa91400 psiASTM D 882
1% Secant Modulus, TD 900 MPa131000 psiASTM D 882
 
Thermal PropertiesMetricEnglishComments
Vicat Softening Point 125 °C257 °FASTM D 1525
 
Descriptive Properties
Low Friction Puncture (J/mm)23NOVA Chemicals Test Method
Moisture Vapor Transmission Rate (g/m²/24h)4At 38°C, 100% RH

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Tabriz HD 6070EA High Density Polyethylene Copolymer
Amco PRIMATOP HDPE 002955 Phillips Process Hexene Copolymer
Braskem Flexus® 7200 Cast Film Extrusion Polyethylene
Iran Petrochemical (PCC) EX 4 HM9455 F High Density Polyethylene
DuPont Teijin Films Mylar® HS Polyester Film, 150 Gauge (38 µm)

PNOV860 / 108467

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.