MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
NOVA Chemicals Sclair® 17A Butene HDPE Film Resin
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Film Grade

Material Notes: 17A complies with the U.S. FDA specifications for olefin polymers and may thus be used in the United States as an article or component of an article intended for use in contact with food, without temperature or food-type restrictions, subject to technical suitability.

NOVA Chemicals' polyethylene resins are chemically and biologically inert.

Features: Low gel, Good processability

Additives: Process stabilizer

Applications: Co-extrusions, Blending

Properties measured from film produced on a laboratory extruder with a 4 inch die, 35 mil die gap, and a BUR of 2.5:1

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.950 g/ccASTM D 792
Oxygen Transmission Rate 1920 cc/m²/day0% RH; ASTM D 1434
Thickness 38.0 microns
Melt Flow 0.45 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D 1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 67ASTM D 2240
Film Tensile Strength at Yield, MD 22.0 MPaASTM D 882
Film Tensile Strength at Yield, TD 20.0 MPaASTM D 882
Film Elongation at Break, MD 650 %ASTM D 882
Film Elongation at Break, TD 750 %ASTM D 882
Coefficient of Friction 0.24ASTM D 1894
Elmendorf Tear Strength MD 22 gASTM D 1922
Elmendorf Tear Strength TD 875 gASTM D 1922
Elmendorf Tear Strength, MD 0.600 g/micronASTM D 1922
Elmendorf Tear Strength, TD 23.0 g/micron
Dart Drop Test 40.0 g1.1; ASTM D 1709/A
Film Tensile Strength at Break, MD 45.0 MPaASTM D 882
Film Tensile Strength at Break, TD 20.0 MPaASTM D 882
1% Secant Modulus, MD 630 MPaASTM D 882
1% Secant Modulus, TD 900 MPaASTM D 882
 
Thermal PropertiesOriginal ValueComments
Vicat Softening Point 125 °CASTM D 1525
 
Descriptive Properties
Low Friction Puncture (J/mm)23NOVA Chemicals Test Method
Moisture Vapor Transmission Rate (g/m²/24h)4At 38°C, 100% RH

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Tabriz HD 6070EA High Density Polyethylene Copolymer
Amco PRIMATOP HDPE 002955 Phillips Process Hexene Copolymer
Braskem Flexus® 7200 Cast Film Extrusion Polyethylene
Iran Petrochemical (PCC) EX 4 HM9455 F High Density Polyethylene
DuPont Teijin Films Mylar® HS Polyester Film, 150 Gauge (38 µm)

PNOV860 / 108467

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.