MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Schott ZERODUR® Glass Ceramic
Categories: Ceramic; Glass; Optical

Material Notes: ZERODUR® is a glass ceramic with an extremely low thermal expansion for demanding applications in which geometrical shape and distance changes must kept smallest possible under temperature variations. The key properties of ZERODUR® are:
  • Extremely low coefficient of thermal expansion (CTE) for a wide temperature range
  • Excellent CTE homogeneity throughout the total volume
  • Very low content of imperfections
  • Wide range of precise geometrical Shapes
  • Extremely smooth surface with residual roughness below 1 nm
Uses:
  • Stages and mirrors for lithography equipment
  • Mirror substrates for segmented and monolithic large astronomical telescopes
  • Ultra light weighted mirror blanks
  • High precision mechanical parts, e.g. ring laser gyroscope bodies
  • Reference standards for precision measurement technology and comet probes

Information provided by SCHOTT.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 2.53 g/cc0.0914 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Knoop 6206200.1/20
Modulus of Elasticity 90.3 GPa13100 ksi
Poissons Ratio 0.240.24
Shear Modulus 36.4 GPa5280 ksiCalculated
 
Thermal PropertiesMetricEnglishComments
CTE, linear  0.000 - 0.00700 µm/m-°C
@Temperature 0.000 - 50.0 °C
0.000 - 0.00389 µin/in-°F
@Temperature 32.0 - 122 °F
EXTREME
 0.000 - 0.0100 µm/m-°C
@Temperature 0.000 - 50.0 °C
0.000 - 0.00556 µin/in-°F
@Temperature 32.0 - 122 °F
SPECIAL
 0.000 - 0.0200 µm/m-°C
@Temperature 0.000 - 50.0 °C
0.000 - 0.0111 µin/in-°F
@Temperature 32.0 - 122 °F
class 0
 0.0100 - 0.0300 µm/m-°C
@Temperature 0.000 - 50.0 °C
0.00556 - 0.0167 µin/in-°F
@Temperature 32.0 - 122 °F
Homogeneity
 0.000 - 0.0500 µm/m-°C
@Temperature 0.000 - 50.0 °C
0.000 - 0.0278 µin/in-°F
@Temperature 32.0 - 122 °F
class 1
 0.000 - 0.100 µm/m-°C
@Temperature 0.000 - 50.0 °C
0.000 - 0.0556 µin/in-°F
@Temperature 32.0 - 122 °F
class 2
Specific Heat Capacity 0.800 J/g-°C0.191 BTU/lb-°F
Thermal Conductivity 1.45 W/m-K10.1 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 600 °C1110 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Schott ZERODUR® K20 Glass Ceramic
Mateck Zero Expansion Glass - ZERODUR
CeramTec Sikor® S Cordierite
Carpenter Invar 36® Alloy, Cold Drawn Bars
Delrin Delrin® 150 NC010 POM

CSGT9948 / 183201

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.