MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

CeramTec Rubalit® 710 Alumina, 99.6%
Categories: Ceramic; Oxide; Aluminum Oxide

Material Notes: Rubalit® 710 (99.6%) is an alumina that produces optimum results and is considered the material of choice for thin-film technology. Its characterizing features are high strength and thermal conductivity.

Key Words: Al2O3, aluminum oxide
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 3.90 g/cc0.141 lb/in³DIN EN 623-2 / ASTM-C373 / ASTM-C20
Water Absorption 0.00 %0.00 %DIN EN 623-2 / ASTM-C373
Particle Size 2.0 µm2.0 µmMedian Grain (d50)
 
Mechanical PropertiesMetricEnglishComments
Tensile Modulus 350 GPa50800 ksiYoung's; DINV ENV 843-2 / ASTM-F417
Flexural Strength 400 MPa58000 psiBending Strength; Dual Ring Method (0.63 mm Substrate Thickness); DIN 52292
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity  1.00e+9 ohm-cm
@Temperature 900 °C
1.00e+9 ohm-cm
@Temperature 1650 °F
 1.00e+13 ohm-cm
@Temperature 25.0 °C
1.00e+13 ohm-cm
@Temperature 77.0 °F
ASTM-D257
 1.00e+13 ohm-cm
@Temperature 500 °C
1.00e+13 ohm-cm
@Temperature 932 °F
Dielectric Constant  10.1
@Frequency 1e+6 Hz
10.1
@Frequency 1e+6 Hz
IEC 672-1 / ASTM-C150
 10.1
@Frequency 1e+9 Hz
10.1
@Frequency 1e+9 Hz
IEC 672-1 / ASTM-C150
Dielectric Breakdown >= 10000 V
@Thickness 1.00 mm
>= 10000 V
@Thickness 0.0394 in
Dielectric Loss Index 0.00020
@Frequency 1e+6 Hz
0.00020
@Frequency 1e+6 Hz
IEC 672-1 / ASTM-D149,150
 
Thermal PropertiesMetricEnglishComments
CTE, linear  6.80 µm/m-°C
@Temperature 20.0 - 200 °C
3.78 µin/in-°F
@Temperature 68.0 - 392 °F
 7.50 µm/m-°C
@Temperature 20.0 - 600 °C
4.17 µin/in-°F
@Temperature 68.0 - 1110 °F
ASTM-C373
 8.50 µm/m-°C
@Temperature 20.0 - 1000 °C
4.72 µin/in-°F
@Temperature 68.0 - 1830 °F
Thermal Conductivity 28.0 W/m-K194 BTU-in/hr-ft²-°FDIN EN 821-2 / ASTM-C408
 
Component Elements PropertiesMetricEnglishComments
Al2O3 99.6 %99.6 %
 
Descriptive Properties
ColorWhite
Ra = Arithmetic Mean Roughness Value (µm)Profilometer (0.8 mm Cutoff)
Te Value (°C)> 1000

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
CeramTec Rubalit® 708S Alumina, 96%
CoorsTek Superstrate® 996 99.6% Alumina Thin Film
CeramTec AT 79 Alumina, 99.6%
CeramTec Rubalit® 702 Alumina, 85%
Arc Cast Molybdenum TZM (Mo-0.5Ti-0.1Zr; Mo alloy 363), Stress Relieved

CCERA933 / 107533

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.