MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

EMS-Grivory Grilon® BS V0 PA6
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6)

Material Notes: Product description: Grilon BS V0 is an unreinforced, normal viscosity, self-extinguishing PA6 injection molding grade. Grilon BS V0 has the following important properties:
  • Halogen and phosphorous-free
  • Light natural color
  • UL94 V-0 at 0.25 mm wall thickness
  • Good electrical properties
Grilon BS V0 is used typically in electrical applications such are switches, plugs, clamps, and connectors.

Information provided by EMS Grivory.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.16 g/cc0.0419 lb/in³Dry; ISO 1183
Water Absorption 8.0 %8.0 %Sim. to ISO 62
Moisture Absorption 2.50 %2.50 %Sim. to ISO 62
Linear Mold Shrinkage, Flow 0.0080 cm/cm0.0080 in/inISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.0090 cm/cm0.0090 in/inISO 294-4, 2577
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 55.0 MPa7980 psiConditioned; ISO 527-1/-2
 70.0 MPa10200 psiDry; ISO 527-1/-2
Tensile Strength, Yield 45.0 MPa6530 psiConditioned; ISO 527-1/-2
 90.0 MPa13100 psiDry; ISO 527-1/-2
Elongation at Break 4.0 %4.0 %Dry; ISO 527-1/-2
 >= 50 %>= 50 %Conditioned; ISO 527-1/-2
Elongation at Yield 3.0 %3.0 %Dry; ISO 527-1/-2
 15 %15 %Conditioned; ISO 527-1/-2
Tensile Modulus 1.20 GPa174 ksiConditioned; ISO 527-1/-2
 3.70 GPa537 ksiDry; ISO 527-1/-2
Charpy Impact Unnotched  NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
Conditioned; ISO 179/1eU
 NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
Dry; ISO 179/1eU
Charpy Impact, Notched  0.300 J/cm²
@Temperature 23.0 °C
1.43 ft-lb/in²
@Temperature 73.4 °F
Dry; ISO 179/1eA
 1.50 J/cm²
@Temperature 23.0 °C
7.14 ft-lb/in²
@Temperature 73.4 °F
Conditioned; ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+10 ohm-cm1.00e+10 ohm-cmConditioned; IEC 60093
 1.00e+12 ohm-cm1.00e+12 ohm-cmDry; IEC 60093
Surface Resistance 1.00e+11 ohm1.00e+11 ohmIEC 60093
Dielectric Constant  3.0
@Frequency 100 Hz
3.0
@Frequency 100 Hz
Dry; IEC 60250
 4.0
@Frequency 1e+6 Hz
4.0
@Frequency 1e+6 Hz
Dry; IEC 60250
 4.0
@Frequency 1e+6 Hz
4.0
@Frequency 1e+6 Hz
Conditioned; IEC 60250
 8.0
@Frequency 100 Hz
8.0
@Frequency 100 Hz
Conditioned; IEC 60250
Dielectric Strength 29.0 kV/mm737 kV/inConditioned; IEC 60243-1
 32.0 kV/mm813 kV/inDry; IEC 60243-1
Dissipation Factor  0.0030
@Frequency 100 Hz
0.0030
@Frequency 100 Hz
Dry; IEC 60250
 0.020
@Frequency 1e+6 Hz
0.020
@Frequency 1e+6 Hz
Dry; IEC 60250
 0.085
@Frequency 1e+6 Hz
0.085
@Frequency 1e+6 Hz
Conditioned; IEC 60250
 0.10
@Frequency 100 Hz
0.10
@Frequency 100 Hz
Conditioned; IEC 60250
Comparative Tracking Index 575 V575 VConditioned; IEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 70.0 µm/m-°C38.9 µin/in-°FISO 11359-1/-2
CTE, linear, Transverse to Flow 90.0 µm/m-°C50.0 µin/in-°FISO 11359-1/-2
Melting Point 222 °C432 °F10°C/min; ISO 11357-1/-3
Maximum Service Temperature, Air 100 - 120 °C212 - 248 °FLong Term; ISO 2578
 180 °C356 °FShort Term; EMS
Deflection Temperature at 0.46 MPa (66 psi) 170 °C338 °FISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 70.0 °C158 °FISO 75-1/-2
Flammability, UL94 V-0V-0IEC 60695-11-10
 V-0
@Temperature 1.50 °C
V-0
@Temperature 34.7 °F
IEC 60695-11-10
Oxygen Index 32 %32 %ISO 4589-1/-2
 
Descriptive Properties
AutomotiveAutomotive electr. and electronics, lighting
Electricals & ElectronicsCables & Tubes
 Connectors
 Electrical appliances
 Electrical equipment
 Energy distribution
 Lighting
FormGranules
ProcessingInjection Molding
Product AttributesNucleated
Special CharacteristicsFlame retardant

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Celanese Nilit Nilamid B FR HF Unfilled, Flame Retardant, Halogen and Red Phosphorous Free PA6
Domo TECHNYL® C 50 H2 PA6, DRY
Envalior Akulon® K225-KWS (Dry) Nylon 6 (North America)
EMS-Grivory Grilon® AS V0 PA66
EMS-Grivory Grilon® TS V0 PA666

PGRH217 / 156926

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.