MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Phillips Sumika Marlex® AGM-250 Polypropylene Impact Copolymer, Ultra-low temperature, impact-resistant, reactor TPO  (discontinued **)
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene Copolymer

Material Notes: Applications: Automotive Interior Trim

Information provided by Phillips Sumika Polypropylene Company (PSPC).

Phillips Sumika Polypropylene Company has been shut down, as announced in 2011.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.900 g/cc
@Thickness 3.17 mm
0.0325 lb/in³
@Thickness 0.125 in
injection-molded specimen; ASTM D1505
Melt Flow 25 g/10 min
@Load 2.16 kg,
Temperature 230 °C
25 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 80
@Thickness 3.17 mm
80
@Thickness 0.125 in
injection-molded specimen; ASTM D785
Tensile Strength, Yield 21.5 MPa
@Thickness 3.17 mm
3120 psi
@Thickness 0.125 in
Type 1 Specimen, Rate: 2"/min; injection-molded specimen; ASTM D638
Flexural Modulus 1.20 GPa
@Thickness 3.17 mm
174 ksi
@Thickness 0.125 in
Tangent; Rate 0.5"/min; injection-molded specimen; ASTM D790
Izod Impact, Notched 1.40 J/cm
@Thickness 3.17 mm
2.62 ft-lb/in
@Thickness 0.125 in
injection molded specimen; ASTM D256
 0.530 J/cm
@Thickness 3.17 mm,
Temperature -30.0 °C
0.993 ft-lb/in
@Thickness 0.125 in,
Temperature -22.0 °F
injection-molded specimen; ASTM D256
 0.850 J/cm
@Thickness 3.17 mm,
Temperature 0.000 °C
1.59 ft-lb/in
@Thickness 0.125 in,
Temperature 32.0 °F
injection-molded specimen; ASTM D256
Dart Drop, Total Energy 38.0 J
@Temperature -30.0 °C
28.0 ft-lb
@Temperature -22.0 °F
150 in/sec; ASTM D3763
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 96.0 °C
@Thickness 3.17 mm
205 °F
@Thickness 0.125 in
injection molded specimen; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 58.0 °C
@Thickness 3.17 mm
136 °F
@Thickness 0.125 in
injection molded specimen; ASTM D648

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
LyondellBasell Pro-fax™ SG899 Polypropylene Copolymer
Phillips Sumika Marlex® AGN-200 Polypropylene Impact Copolymer
Phillips Sumika Marlex® AGX-230 Polypropylene Impact Copolymer
ExxonMobil PP4031E2 Polypropylene Impact Copolymer
ExxonMobil PP7011L1 Polypropylene Impact Copolymer

PCHEVS0m / 20354

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.