MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Greene Tweed Xyfluor® 860 Fluorinated Elastomer Compound
Categories: Polymer; Thermoset; Fluoropolymer, TS; Thermoset Fluoroelastomer; Rubber or Thermoset Elastomer (TSE)

Material Notes: Xyfluor® 860, a highly fluorinated elastomer compound, offers excellent chemical compatibility over a wide range of temperatures from -76°F to 450°F (-60°C to 232°C). Recommended for applications requiring a combination of low-temperature properties and chemical resistance, Xyfluor’s capabilities surpass those of standard fluoroelastomers, PTFE, and graphite. Additionally, Xyfluor reduces overall cost by extending equipment service life.

Applications:Xyfluor works well in demanding applications such as mechanical seals, gaskets and other custom components in a variety of metering pumps, valves and other high-performance equipment.

Information provided by Greene Tweed.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 7070ASTM D2240
Tensile Strength at Break 6.89 MPa1000 psiASTM D1414
Tensile Strength, Yield 2.41 MPa350 psi@100% Elongation; ASTM D1414
Elongation at Break 250 %250 %ASTM D1414
Compression Set 30 %
@Temperature 204 °C,
Time 252000 sec
30 %
@Temperature 400 °F,
Time 70.0 hour
At 25% deflection; ASTM D395
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 232 °C450 °F
Minimum Service Temperature, Air -60.0 °C-76.0 °F
 
Descriptive Properties
ColorBlack

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Beijing Evergrow Resources PTFE, 20% Glass Fiber, 5% Graphite Filled
Guarniflon PTFE G455 Polytetrafluoroethylene 35% Carbographite
AISI 6150 Steel, annealed, 25 mm (1 in.) round
AISI 4340 Steel, oil quenched 830°C (1525°F), 540°C (1000°F) temper, not nitrided
AGC Fluon® FC168-63 PTFE, 63% Bronze and Graphite Filled

PGREEN47 / 42341

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.