MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Covestro Texin® 985 Thermoplastic Polyurethanes (TPU)
Categories: Polymer; Thermoplastic; Polyurethane, TP

Material Notes: Texin 985 resin is an aromatic polyether-based thermoplastic polyurethane with a Shore hardness of approximately 85A. It can be processed by injection molding, extrusion, or blow molding.

Properties / Applications: Texin 985 resin offers outstanding abrasion resistance, impact strength, toughness, and flexibility. It also exhibits excellent inherent resistance to salt water stress cracking, and hydrolysis. Texin 985 natural color resin complies with FDA food-contact regulations 21 CFR 177.1680 (Polyurethane Resins) and 177.2600 (Rubber Articles Intended for Repeated Use), subject to the limitations of these and any other applicable regulations. In addition, Texin 985 natural color resin is listed under NSF standard 61 for use in potable water applications. Typical applications include gaskets, hose, tubing, shoe inserts, connectors, belting, and miscellaneous molded articles.

Information provided by Covestro

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.12 g/cc1.12 g/ccASTM D792
Linear Mold Shrinkage, Flow 0.0080 cm/cm
@Thickness 2.54 mm
0.0080 in/in
@Thickness 0.100 in
ASTM D955
Linear Mold Shrinkage, Transverse 0.0080 cm/cm
@Thickness 2.54 mm
0.0080 in/in
@Thickness 0.100 in
ASTM D955
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 8585ASTM D2240
Tensile Strength at Break 38.6 MPa5600 psiASTM D412
Tensile Stress at Strain  4.80 MPa
@Strain 50 %
696 psi
@Strain 50 %
ASTM D412
 5.50 MPa
@Strain 100 %
798 psi
@Strain 100 %
ASTM D412
 9.70 MPa
@Strain 300 %
1410 psi
@Strain 300 %
ASTM D412
Elongation at Break 590 %590 %ASTM D412
Flexural Modulus  0.0269 GPa
@Thickness 584 mm
3.90 ksi
@Thickness 23.0 in
ASTM D790
 0.0590 GPa
@Thickness -762 mm
8.56 ksi
@Thickness -30.0 in
ASTM D790
Compressive Strength 0.300 MPa43.5 psi2% Deflection; ASTM D 575
 1.00 MPa145 psi5% Deflection; ASTM D 575
 2.10 MPa305 psi10% Deflection; ASTM D 575
 3.10 MPa450 psi15% Deflection; ASTM D 575
 4.30 MPa624 psi20% Deflection; ASTM D 575
 5.50 MPa798 psi25% Deflection; ASTM D 575
 16.5 MPa2390 psi50% Deflection; ASTM D 575
Resilience 4545[%], Bayshore; ASTM D2632
Tear Strength 87.6 kN/m500 pliDie C; ASTM D624
Taber Abrasion, mg/1000 Cycles 30
@Load 1.00 kg
30
@Load 2.20 lb
[mg] Loss, H-18; ASTM D3489
Compression Set  16 %
@Temperature 23.0 °C,
Time 79200 sec
16 %
@Temperature 73.4 °F,
Time 22.0 hour
postcured; ASTM D395-B
 19 %
@Temperature 23.0 °C,
Time 79200 sec
19 %
@Temperature 73.4 °F,
Time 22.0 hour
as molded; ASTM D395-B
 40 %
@Temperature 70.0 °C,
Time 79200 sec
40 %
@Temperature 158 °F,
Time 22.0 hour
postcured; ASTM D395-B
 80 %
@Temperature 70.0 °C,
Time 79200 sec
80 %
@Temperature 158 °F,
Time 22.0 hour
as molded; ASTM D395-B
 
Thermal PropertiesMetricEnglishComments
Vicat Softening Point 80.0 °C176 °FRate A; ASTM D1525
Brittleness Temperature >= -55.6 °C>= -68.0 °FASTM D746
Glass Transition Temp, Tg -46.0 °C-50.8 °F
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 177 - 193 °C351 - 379 °F
Middle Barrel Temperature 182 - 199 °C360 - 390 °F
Front Barrel Temperature 182 - 204 °C360 - 399 °F
Nozzle Temperature 185 - 207 °C365 - 405 °F
Zone 1 182 - 199 °C360 - 390 °FExtrusion
Zone 2 182 - 204 °C360 - 399 °FExtrusion
Zone 3 182 - 210 °C360 - 410 °FExtrusion
Die Temperature 188 - 210 °C370 - 410 °FExtrusion
Melt Temperature 190 - 205 °C374 - 401 °FExtrusion
 193 - 210 °C379 - 410 °FInjection
Mold Temperature 16.0 - 43.0 °C60.8 - 109 °F
Injection Pressure 41.4 - 103 MPa6000 - 15000 psiInjection
Hold Pressure 27.6 - 55.2 MPa4000 - 8000 psiInjection
Back Pressure <= 5.52 MPa<= 800 psiInjection
Cushion 0.317 - 0.635 cm0.125 - 0.250 inInjection
 
Compliance PropertiesMetricEnglishComments
FDA YesYes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Covestro Texin® 985 U Thermoplastic Polyurethanes (TPU)
Lubrizol ESTANE® 58887 Ether Based Thermoplastic Polyurethane
Covestro Texin® RxT70A Thermoplastic Polyurethanes (TPU)
Covestro Texin® 4215 Thermoplastic Polyurethanes (TPU)
Covestro Texin® 245 Thermoplastic Polyurethanes (TPU)

PCOVEST0983 / 202766

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.