MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Covestro Texin® RxT70A Thermoplastic Polyurethanes (TPU)
Categories: Polymer; Thermoplastic; Polyurethane, TP

Material Notes: Characterization: Texin RxT70A resin is an aromatic polyether-based thermoplastic polyurethane. It can be processed by injection molding or extrusion.

Properties / Applications: Texin RxT70A is characterized by very good hydrolysis, good low temperature flexibility, resiliency and impact strength, high moisture vapor transmission rates and is plasticizer free. Typical medical applications include catheters and catheter balloons, specialty tubing and profiles, connectors, and soft overmolding applications. As with any product, the use of Texin RxT70A resin in a given application must be tested (including but not limited to field testing) in advance by the user to determine suitability.

Information provided by Covestro

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.07 g/cc1.07 g/ccASTM D792
Linear Mold Shrinkage, Flow 0.0080 cm/cm
@Thickness 2.54 mm
0.0080 in/in
@Thickness 0.100 in
ASTM D955
Linear Mold Shrinkage, Transverse 0.0080 cm/cm
@Thickness 2.54 mm
0.0080 in/in
@Thickness 0.100 in
ASTM D955
Melt Flow 32 g/10 min
@Load 10.0 kg,
Temperature 200 °C
32 g/10 min
@Load 22.0 lb,
Temperature 392 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 7070ASTM D2240
Tensile Strength at Break 25.5 MPa3700 psiASTM D412
Tensile Stress at Strain  3.40 MPa
@Strain 100 %
493 psi
@Strain 100 %
ASTM D412
 5.20 MPa
@Strain 300 %
754 psi
@Strain 300 %
ASTM D412
Elongation at Break 770 %770 %ASTM D412
Flexural Modulus 0.0145 GPa2.10 ksiASTM D790
Tear Strength 60.5 kN/m345 pliDie C; ASTM D624
Taber Abrasion, mg/1000 Cycles 7.0
@Load 1.00 kg
7.0
@Load 2.20 lb
[mg] Loss, H-18; ASTM D3489
Compression Set  11 %
@Temperature 23.0 °C,
Time 79200 sec
11 %
@Temperature 73.4 °F,
Time 22.0 hour
postcured; ASTM D395-B
 30 %
@Temperature 70.0 °C,
Time 79200 sec
30 %
@Temperature 158 °F,
Time 22.0 hour
postcured; ASTM D395-B
 
Thermal PropertiesMetricEnglishComments
Vicat Softening Point 75.0 °C167 °FRate A; ASTM D1525
 
Optical PropertiesMetricEnglishComments
Yellow Index <= 15 %<= 15 %ASTM E313
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 182 - 193 °C360 - 379 °FInjection
 182 - 199 °C360 - 390 °FExtrusion
Middle Barrel Temperature 182 - 204 °C360 - 399 °FExtrusion
 188 - 199 °C370 - 390 °FInjection
Front Barrel Temperature 182 - 204 °C360 - 399 °FExtrusion
 188 - 199 °C370 - 390 °FInjection
Nozzle Temperature 191 - 202 °C376 - 396 °FInjection
Die Temperature 188 - 204 °C370 - 399 °FExtrusion
Melt Temperature 188 - 199 °C370 - 390 °FInjection
 191 - 204 °C376 - 399 °FExtrusion
Mold Temperature 16.0 - 38.0 °C60.8 - 100 °FInjection
Injection Pressure 41.4 - 103 MPa6000 - 15000 psiInjection
Back Pressure <= 1.38 MPa<= 200 psiInjection
Cushion <= 0.317 cm<= 0.125 inInjection

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Covestro Texin® 1209 Thermoplastic Polyurethanes (TPU)
Covestro Texin® 985 Thermoplastic Polyurethanes (TPU)
Covestro Texin® 270 Thermoplastic Polyurethanes (TPU)
Covestro Texin® 970 U Thermoplastic Polyurethanes (TPU)
Trinseo EMERGE™ 9500CR Polycarbonate (PC) / Polyethylene Terephthalate (PET)

PCOVEST0997 / 202780

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.