MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Envalior Pocan® DP C 1502 000000 PBT+PC
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Unreinforced

Material Notes: PBT+PC, non-reinforced, improved toughness, reduced warpage

Former Lanxess product line is now with Envalior.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.21 g/cc0.0437 lb/in³ISO 1183
Linear Mold Shrinkage, Flow 0.012 cm/cm0.012 in/inPlaque 60 x 60 x 2mm; ISO 294-4
Linear Mold Shrinkage, Transverse 0.012 cm/cm0.012 in/inPlaque 60 x 60 x 2mm; ISO 294-4
Melt Flow 35 g/10 min
@Load 5.00 kg,
Temperature 270 °C
35 g/10 min
@Load 11.0 lb,
Temperature 518 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 50.0 MPa7250 psi50 mm/min; ISO 527-1,-2
Elongation at Break >= 40 %>= 40 %Nominal, 50 mm/min; ISO 527-1,-2
Elongation at Yield 3.8 %3.8 %50 mm/min; ISO 527-1,-2
Tensile Modulus 2.10 GPa305 ksi1 mm/min; ISO 527-1,-2
Flexural Yield Strength 65.0 MPa
@Strain 3.5 %
9430 psi
@Strain 3.5 %
2 mm/min; ISO 178-A
Flexural Strain at Yield 5.5 %5.5 %2 mm/min; ISO 178-A
Izod Impact, Notched (ISO)  17.0 kJ/m²
@Temperature -30.0 °C
8.09 ft-lb/in²
@Temperature -22.0 °F
ISO 180-1A
 60.0 kJ/m²
@Temperature 23.0 °C
28.6 ft-lb/in²
@Temperature 73.4 °F
ISO 180-1A
Izod Impact, Unnotched (ISO)  NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
ISO 180-1U
 NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
ISO 180-1U
Charpy Impact Unnotched  NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
ISO 179-1eU
 NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
ISO 179-1eU
Charpy Impact, Notched  1.90 J/cm²
@Temperature -30.0 °C
9.04 ft-lb/in²
@Temperature -22.0 °F
ISO 179-1eA
 6.00 J/cm²
@Temperature 23.0 °C
28.6 ft-lb/in²
@Temperature 73.4 °F
ISO 179-1eA
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 110 µm/m-°C
@Temperature 23.0 - 55.0 °C
61.1 µin/in-°F
@Temperature 73.4 - 131 °F
ISO 11359-1,-2
CTE, linear, Transverse to Flow 110 µm/m-°C
@Temperature 23.0 - 55.0 °C
61.1 µin/in-°F
@Temperature 73.4 - 131 °F
ISO 11359-1,-2
Melting Point 225 °C437 °F10°C/min; ISO 11357-1,-3
Deflection Temperature at 0.46 MPa (66 psi) 70.0 °C158 °FMethod Af; ISO 75-1,-2
Deflection Temperature at 1.8 MPa (264 psi) 105 °C221 °FMethod Bf; ISO 75-1,-2
Flammability, UL94 HB
@Thickness 0.750 mm
HB
@Thickness 0.0295 in
UL Yellow Card
Glow Wire Flammability Index 750 °C
@Thickness 4.00 mm
1380 °F
@Thickness 0.157 in
IEC 60695-2-12
 
Processing PropertiesMetricEnglishComments
Melt Temperature 250 °C482 °FPlaque 60 x 60 x 2mm
Mold Temperature 70.0 °C158 °FPlaque 60 x 60 x 2mm
Hold Pressure 60.0 MPa8700 psiPlaque 60 x 60 x 2mm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Envalior Pocan® DP CF 2200 000000 PBT+PC
Overview of materials for Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Unreinforced
Covestro Makroblend® UT3907 PC+PBT
Covestro Makroblend® UT6007 PC+PBT
Barlog Plastics KEBATER A1100 PBT/PC unreinforced, high impact

PLANW9011 / 208438

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.