MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Covestro Apec® HT KU 1-9357/2 High-Heat Polycarbonate, 20% Glass Fiber
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate, Glass Fiber Filled, Flame Retardant

Material Notes: Only opaque colors available, with 20% glass fiber reinforcement, flame retardant.

Applications: Lighting, electrical parts.

Information provided by Bayer.

As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covestro.

Key Words: PC
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.30 g/cc0.0470 lb/in³
Moisture Absorption at Equilibrium 0.15 %0.15 %50% RH
Water Absorption at Saturation 0.35 %0.35 %
 0.35 %0.35 %
Melt Flow 6.0 g/10 min
@Load 2.16 kg,
Temperature 330 °C
6.0 g/10 min
@Load 4.76 lb,
Temperature 626 °F
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 100 MPa14500 psi
Elongation at Break 3.0 %3.0 %
Tensile Modulus 5.90 GPa856 ksi
Charpy Impact Unnotched 5.00 J/cm²23.8 ft-lb/in²
 0.800 J/cm²
@Temperature -30.0 °C
3.81 ft-lb/in²
@Temperature -22.0 °F
Charpy Impact, Notched 0.800 J/cm²3.81 ft-lb/in²
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity >= 1.00e+15 ohm-cm>= 1.00e+15 ohm-cm
Surface Resistance >= 1.00e+15 ohm>= 1.00e+15 ohm
Dielectric Constant  3.1
@Frequency 1e+6 Hz
3.1
@Frequency 1e+6 Hz
 3.2
@Frequency 100 Hz
3.2
@Frequency 100 Hz
Dielectric Strength 38.0 kV/mm965 kV/in
Dissipation Factor  0.0015
@Frequency 100 Hz
0.0015
@Frequency 100 Hz
 0.0088
@Frequency 1e+6 Hz
0.0088
@Frequency 1e+6 Hz
Comparative Tracking Index 200 V200 V
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 30.0 µm/m-°C
@Temperature 20.0 °C
16.7 µin/in-°F
@Temperature 68.0 °F
CTE, linear, Transverse to Flow 60.0 µm/m-°C
@Temperature 20.0 °C
33.3 µin/in-°F
@Temperature 68.0 °F
Deflection Temperature at 0.46 MPa (66 psi) 184 °C363 °F
Deflection Temperature at 1.8 MPa (264 psi) 178 °C352 °F
Vicat Softening Point 186 °C367 °F
Flammability, UL94  V-0
@Thickness 1.60 mm
V-0
@Thickness 0.0630 in
 V-0
@Thickness 3.00 mm
V-0
@Thickness 0.118 in

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Covestro Apec® HT KU 1-9371 High-Heat Polycarbonate
Covestro Makrolon® GF8001 Polycarbonate, 20% Glass Filled
Arkema Orgalloy® RS 6010 NAT Polyamide 6 Alloy 10% Glass Fiber reinforced
Covestro Apec® HT KU 1-9373 High-Heat Polycarbonate
Avient Edgetek® ET3500-5002 BK Acrylonitrile Styrene Acrylate + PC (ASA+PC)

PBA011 / 26647

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.