MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Constellium DOKIMA® Rolled Plate Aluminum
Categories: Metal; Nonferrous Metal; Aluminum Alloy; 6000 Series Aluminum Alloy

Material Notes: DOKIMA® rolled plates have moderate strength properties, a very low level of impurities, an excellent corrosion resistance, a very good dimensional stability and high thermal and electrical conductivity. DOKIMA® is recommended for sensitive applications in nuclear, pharmaceutical, food, semi-conductor and telecommunication industries.

Information provided by manufacturer

Key Words: Alloy 6063S
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 2.69 g/cc0.0972 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell  100
@Thickness 8.00 - 25.0 mm
100
@Thickness 0.315 - 0.984 in
 100
@Thickness 25.0 - 60.0 mm
100
@Thickness 0.984 - 2.36 in
 100
@Thickness 60.0 - 100 mm
100
@Thickness 2.36 - 3.94 in
 100
@Thickness 100 - 150 mm
100
@Thickness 3.94 - 5.91 in
Tensile Strength  >= 260 MPa
@Thickness 8.00 - 25.0 mm
>= 37700 psi
@Thickness 0.315 - 0.984 in
Temper T651
 >= 260 MPa
@Thickness 25.0 - 60.0 mm
>= 37700 psi
@Thickness 0.984 - 2.36 in
Temper T651
 >= 260 MPa
@Thickness 60.0 - 150 mm
>= 37700 psi
@Thickness 2.36 - 5.91 in
Temper T651
 300 MPa
@Thickness 8.00 - 25.0 mm
43500 psi
@Thickness 0.315 - 0.984 in
Typical Strength
 300 MPa
@Thickness 25.0 - 60.0 mm
43500 psi
@Thickness 0.984 - 2.36 in
Typical Strength
 300 MPa
@Thickness 60.0 - 100 mm
43500 psi
@Thickness 2.36 - 3.94 in
Typical Strength
 300 MPa
@Thickness 100 - 150 mm
43500 psi
@Thickness 3.94 - 5.91 in
Typical Strength
Tensile Strength, Yield  >= 220 MPa
@Strain 0.2 %,
Thickness 8.00 - 25.0 mm
>= 31900 psi
@Strain 0.2 %,
Thickness 0.315 - 0.984 in
Temper T651
 >= 220 MPa
@Strain 0.2 %,
Thickness 25.0 - 60.0 mm
>= 31900 psi
@Strain 0.2 %,
Thickness 0.984 - 2.36 in
Temper T651
 >= 220 MPa
@Strain 0.2 %,
Thickness 60.0 - 150 mm
>= 31900 psi
@Strain 0.2 %,
Thickness 2.36 - 5.91 in
Temper T651
 260 MPa
@Strain 0.2 %,
Thickness 8.00 - 25.0 mm
37700 psi
@Strain 0.2 %,
Thickness 0.315 - 0.984 in
Typical Strength
 260 MPa
@Strain 0.2 %,
Thickness 25.0 - 60.0 mm
37700 psi
@Strain 0.2 %,
Thickness 0.984 - 2.36 in
Typical Strength
 260 MPa
@Strain 0.2 %,
Thickness 60.0 - 100 mm
37700 psi
@Strain 0.2 %,
Thickness 2.36 - 3.94 in
Typical Strength
 260 MPa
@Strain 0.2 %,
Thickness 100 - 150 mm
37700 psi
@Strain 0.2 %,
Thickness 3.94 - 5.91 in
Typical Strength
Elongation at Break  >= 5.0 %
@Thickness 60.0 - 150 mm
>= 5.0 %
@Thickness 2.36 - 5.91 in
Temper T651
 >= 6.0 %
@Thickness 25.0 - 60.0 mm
>= 6.0 %
@Thickness 0.984 - 2.36 in
Temper T651
 >= 7.0 %
@Thickness 8.00 - 25.0 mm
>= 7.0 %
@Thickness 0.315 - 0.984 in
Temper T651
 8.0 %
@Thickness 100 - 150 mm
8.0 %
@Thickness 3.94 - 5.91 in
Typical Elongation
 9.0 %
@Thickness 60.0 - 100 mm
9.0 %
@Thickness 2.36 - 3.94 in
Typical Elongation
 10 %
@Thickness 8.00 - 25.0 mm
10 %
@Thickness 0.315 - 0.984 in
Typical Elongation
 10 %
@Thickness 25.0 - 60.0 mm
10 %
@Thickness 0.984 - 2.36 in
Typical Elongation
Modulus of Elasticity 68.3 GPa9910 ksi
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00000340 ohm-cm0.00000340 ohm-cmTemper T651
 
Thermal PropertiesMetricEnglishComments
CTE, linear 23.4 µm/m-°C
@Temperature 20.0 - 100 °C
13.0 µin/in-°F
@Temperature 68.0 - 212 °F
Thermal Conductivity 200 W/m-K1390 BTU-in/hr-ft²-°FTemper T651
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al 97.65 - 99.35 %97.65 - 99.35 %as balance
Chromium, Cr <= 0.10 %<= 0.10 %
Copper, Cu <= 0.10 %<= 0.10 %
Iron, Fe <= 0.35 %<= 0.35 %
Magnesium, Mg 0.45 - 0.90 %0.45 - 0.90 %
Manganese, Mn <= 0.10 %<= 0.10 %
Silicon, Si 0.20 - 0.60 %0.20 - 0.60 %
Titanium, Ti <= 0.10 %<= 0.10 %
Zinc, Zn <= 0.10 %<= 0.10 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Superior Flux Superior No. 40MM4 Organic Acid Water-Soluble Flux
Arkema KYNAR® 370 Polyvinylidene Fluoride (PVDF) Homopolymer - Injection Molding
Aluminum 6061-T6; 6061-T651
Goodfellow Aluminum 99/Silicon 1 Alloy
Alpase M-5™ Aluminum Mold Plate

NCONS019 / 160282

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.