MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

LATI Lapex A G/20 PES, 20% Glass Fiber Reinforced
Categories: Polymer; Thermoplastic; Polyethersulfone (PES); Polyethersulfone (PES), 20%Glass Fiber Filled

Material Notes: Polyether Sulfone (PES) based compound. Glass fibers. Low smoke density and low toxicity index. Very high dimensional stability.

Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North America

Information provided by Lati Industria Termoplastici S.p.A.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.49 g/cc0.0538 lb/in³
Linear Mold Shrinkage, Flow 0.0035 - 0.0050 cm/cm0.0035 - 0.0050 in/in
Linear Mold Shrinkage, Transverse 0.0075 - 0.0090 cm/cm0.0075 - 0.0090 in/in
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break  80.0 MPa
@Temperature 150 °C
11600 psi
@Temperature 302 °F
 90.0 MPa
@Temperature 120 °C
13100 psi
@Temperature 248 °F
 100 MPa
@Temperature 90.0 °C
14500 psi
@Temperature 194 °F
 110 MPa
@Temperature 60.0 °C
16000 psi
@Temperature 140 °F
 115 MPa
@Temperature 23.0 °C
16700 psi
@Temperature 73.4 °F
Elongation at Break  2.5 %
@Temperature 23.0 °C
2.5 %
@Temperature 73.4 °F
 2.6 %
@Temperature 60.0 °C
2.6 %
@Temperature 140 °F
 2.7 %
@Temperature 90.0 °C
2.7 %
@Temperature 194 °F
 2.8 %
@Temperature 120 °C
2.8 %
@Temperature 248 °F
 3.0 %
@Temperature 150 °C
3.0 %
@Temperature 302 °F
Elongation at Yield 2.5 %
@Temperature 150 °C
2.5 %
@Temperature 302 °F
Tensile Modulus  5.90 GPa
@Temperature 150 °C
856 ksi
@Temperature 302 °F
 6.15 GPa
@Temperature 120 °C
892 ksi
@Temperature 248 °F
 6.30 GPa
@Temperature 90.0 °C
914 ksi
@Temperature 194 °F
 6.50 GPa
@Temperature 60.0 °C
943 ksi
@Temperature 140 °F
 6.70 GPa
@Temperature 23.0 °C
972 ksi
@Temperature 73.4 °F
Charpy Impact Unnotched 3.50 J/cm²16.7 ft-lb/in²
Charpy Impact, Notched 0.400 J/cm²1.90 ft-lb/in²
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 180 °C356 °F
Deflection Temperature at 0.46 MPa (66 psi) 220 °C428 °F
Deflection Temperature at 1.8 MPa (264 psi) 215 °C419 °F
Vicat Softening Point 220 °C
@Load 5.00 kg
428 °F
@Load 11.0 lb
Flammability, UL94  V-0
@Thickness 3.00 mm
V-0
@Thickness 0.118 in
 V-0
@Thickness 1.50 mm
V-0
@Thickness 0.0591 in
Oxygen Index 39 %39 %
 
Processing PropertiesMetricEnglishComments
Melt Temperature 350 - 370 °C662 - 698 °F
Mold Temperature 140 - 165 °C284 - 329 °F
Drying Temperature 150 - 180 °C
@Time 10800 sec
302 - 356 °F
@Time 3.00 hour
 
Descriptive Properties
ISO Shrinkage - Pressure60 MPa

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
BASF Ultrason® E 2010 G4 20% Glass Filled PES
Gharda Chemicals GAFONE™ 3420GF PES, Glass Fiber-Reinforced
RTP Company RTP 1403 Polyethersulfone (PES), Glass Fiber
Techmer ES HiFill® PES GF20 20% Glass Filled
Overview of materials for Polyethersulfone (PES), 20% Glass Fiber Filled

PLATH9614 / 177310

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.