MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

BASF Ultrason® E 2010 G4 20% Glass Filled PES
Categories: Polymer; Thermoplastic; Polyethersulfone (PES); Polyethersulfone (PES), 20%Glass Fiber Filled

Material Notes: Ultrason E 2010 G4 is a 20% glass reinforced, medium viscosity injection molding PES grade with high rigidity and strength.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.50 g/cc0.0542 lb/in³ISO 1183
Water Absorption 1.6 %1.6 %ISO 62
Moisture Absorption at Equilibrium 0.60 %0.60 %23°C/50% R.H.; ISO 62
Viscosity Number 56 cm³/g0.56 dl/g
Linear Mold Shrinkage, Flow 0.0036 cm/cm0.0036 in/inISO Data
Linear Mold Shrinkage, Transverse 0.0061 cm/cm0.0061 in/inISO Data
Melt Flow 29 g/10 min
@Load 10.0 kg,
Temperature 360 °C
29 g/10 min
@Load 22.0 lb,
Temperature 680 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Ball Indentation Hardness 205 MPa29700 psiISO 2039-1
Tensile Strength at Break 125 MPa18100 psi5mm/min; ISO 527-2
Tensile Strength, Yield 125 MPa18100 psi50mm/min; ISO 527-2
Elongation at Break 2.5 %2.5 %5mm/min; ISO 527-2
Elongation at Yield 2.5 %2.5 %50mm/min; ISO 527-2
Tensile Modulus 7.30 GPa1060 ksiElasticity; ISO 527-2
Shear Modulus  0.200 GPa
@Temperature 225 °C
29.0 ksi
@Temperature 437 °F
ISO 6721
 0.900 GPa
@Temperature 200 °C
131 ksi
@Temperature 392 °F
ISO 6721
 0.950 GPa
@Temperature 100 °C
138 ksi
@Temperature 212 °F
ISO 6721
 1.00 GPa
@Temperature 50.0 °C
145 ksi
@Temperature 122 °F
ISO 6721
Izod Impact, Notched (ISO) 6.50 kJ/m²3.09 ft-lb/in²ISO 180/A
 6.50 kJ/m²
@Temperature -30.0 °C
3.09 ft-lb/in²
@Temperature -22.0 °F
ISO 180/A
Charpy Impact Unnotched 4.70 J/cm²22.4 ft-lb/in²ISO 179/1eU
 4.50 J/cm²
@Temperature -30.0 °C
21.4 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eU
Charpy Impact, Notched 0.650 J/cm²3.09 ft-lb/in²ISO 179/1eA
 0.650 J/cm²
@Temperature -30.0 °C
3.09 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eA
Tensile Creep Modulus, 1000 hours 5600 MPa812000 psiISO 899-1
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+13 ohm-cm>= 1.00e+13 ohm-cmIEC 60093
Surface Resistance >= 1.00e+14 ohm>= 1.00e+14 ohmIEC 60093
Dielectric Constant  4.2
@Frequency 100 Hz
4.2
@Frequency 100 Hz
IEC 60250
 4.2
@Frequency 1e+6 Hz
4.2
@Frequency 1e+6 Hz
IEC 60250
Dielectric Strength 37.0 kV/mm940 kV/inIEC 60243-1
Dissipation Factor  0.0020
@Frequency 100 Hz
0.0020
@Frequency 100 Hz
IEC 60250
 0.010
@Frequency 1e+6 Hz
0.010
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index 125 V125 VTest Liquid A & B; IEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow  20.0 µm/m-°C
@Temperature 23.0 - 80.0 °C
11.1 µin/in-°F
@Temperature 73.4 - 176 °F
ISO 11359-1/-2
 23.0 µm/m-°C
@Temperature 140 - 180 °C
12.8 µin/in-°F
@Temperature 284 - 356 °F
ISO 180/A
Thermal Conductivity 0.190 W/m-K1.32 BTU-in/hr-ft²-°FDIN 52612-1
Maximum Service Temperature, Air 220 °C428 °F
 220 °C428 °Fshort cycle operations
Deflection Temperature at 0.46 MPa (66 psi) 224 °C435 °FISO 75-2
Deflection Temperature at 1.8 MPa (264 psi) 220 °C428 °FISO 75-2
Glass Transition Temp, Tg 225 °C437 °FISO 11357-1/-3
UL RTI, Electrical 180 °C356 °F50% decrease of tensile strength after 20000h; 746B
Flammability, UL94  V-0
@Thickness 1.60 mm
V-0
@Thickness 0.0630 in
 V-0
@Thickness 3.20 mm
V-0
@Thickness 0.126 in
Oxygen Index 44.5 %44.5 %ISO 4589-1/-2
Glow Wire Ignition Temperature 825 °C1520 °FIEC 60695-2-13
Glow Wire Flammability Index 960 °C1760 °FIEC 60695-2-12
 
Processing PropertiesMetricEnglishComments
Melt Temperature 350 - 390 °C662 - 734 °FInjection molding
Mold Temperature 150 - 190 °C302 - 374 °FInjection molding
 
Descriptive Properties
ColorNatural
Commercial StatusNorth America and Europe
Impact ModifiedNo
Primary Processing TechniqueInjection Molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
BASF Ultrason® E 2010 G6 30% Glass Filled PES
BASF Ultrason® S 2010 G4 20% Glass Filled PSU
BASF Ultrason® E 2010 G4 MR SW 15102 20% Glass Filled PESU
BASF Ultrason® E 2010 PES
BASF Ultrason® E 3010 PES

PBASF9400 / 85164

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.