MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

BASF Ultrason® S 2010 G4 20% Glass Filled PSU
Categories: Polymer; Thermoplastic; Polysulfone (PSU); Polysulfone, 20% Glass Fiber Reinforced

Material Notes: Ultrason S 2010 G4 is a 20% glass reinforced, medium viscosity injection molding PSU grade with high rigidity and strength.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.39 g/cc0.0502 lb/in³ISO 1183
Water Absorption 0.70 %0.70 %ISO 62
Moisture Absorption at Equilibrium 0.20 %0.20 %23°C/50% R.H.; ISO 62
Viscosity Number 63 cm³/g0.63 dl/g
Linear Mold Shrinkage, Flow 0.0031 cm/cm0.0031 in/inISO 294
Linear Mold Shrinkage, Transverse 0.0052 cm/cm0.0052 in/inISO 294
Melt Flow 40 g/10 min
@Load 10.0 kg,
Temperature 360 °C
40 g/10 min
@Load 22.0 lb,
Temperature 680 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Ball Indentation Hardness 170 MPa24700 psiISO 2039-1
Tensile Strength at Break 110 MPa16000 psi5mm/min; ISO 527-2
Tensile Strength, Yield 110 MPa16000 psi50mm/min; ISO 527-2
Elongation at Break 2.2 %2.2 %5mm/min; ISO 527-2
Elongation at Yield 2.2 %2.2 %50mm/min; ISO 527-2
Tensile Modulus 6.80 GPa986 ksiISO 527-2
Flexural Strength 164 MPa23800 psiISO Data
Shear Modulus  0.0250 GPa
@Temperature 200 °C
3.63 ksi
@Temperature 392 °F
ISO 6721
 0.800 GPa
@Temperature 175 °C
116 ksi
@Temperature 347 °F
ISO 6721
 0.900 GPa
@Temperature 100 °C
131 ksi
@Temperature 212 °F
ISO 6721
 0.950 GPa
@Temperature 50.0 °C
138 ksi
@Temperature 122 °F
ISO 6721
Izod Impact, Notched (ISO) 7.00 kJ/m²3.33 ft-lb/in²ISO 180/A
 7.00 kJ/m²
@Temperature -30.0 °C
3.33 ft-lb/in²
@Temperature -22.0 °F
ISO 180/A
Charpy Impact Unnotched 4.50 J/cm²21.4 ft-lb/in²ISO 179/1eU
 4.50 J/cm²
@Temperature -30.0 °C
21.4 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eU
Charpy Impact, Notched 0.700 J/cm²3.33 ft-lb/in²ISO 179/1eA
 0.750 J/cm²
@Temperature -30.0 °C
3.57 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eA
Tensile Creep Modulus, 1000 hours 6000 MPa870000 psiISO 899
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+13 ohm-cm>= 1.00e+13 ohm-cmIEC 60093
Surface Resistance >= 1.00e+14 ohm>= 1.00e+14 ohmIEC 60093
Dielectric Constant  3.5
@Frequency 100 Hz
3.5
@Frequency 100 Hz
IEC 60250
 3.5
@Frequency 1e+6 Hz
3.5
@Frequency 1e+6 Hz
IEC 60250
Dielectric Strength 46.0 kV/mm1170 kV/inIEC 60243-1 3
Dissipation Factor  0.0010
@Frequency 100 Hz
0.0010
@Frequency 100 Hz
IEC 60250
 0.0060
@Frequency 1e+6 Hz
0.0060
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index 125 V125 VTest liquid A & B; IEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow  26.0 µm/m-°C
@Temperature 23.0 - 80.0 °C
14.4 µin/in-°F
@Temperature 73.4 - 176 °F
ISO 11359-1/-2
 28.0 µm/m-°C
@Temperature 140 - 180 °C
15.6 µin/in-°F
@Temperature 284 - 356 °F
ISO 11359-1/-2
Maximum Service Temperature, Air 180 °C356 °Fshort cycle operations
Deflection Temperature at 0.46 MPa (66 psi) 188 °C370 °FISO 75
Deflection Temperature at 1.8 MPa (264 psi) 183 °C361 °FISO 75
Glass Transition Temp, Tg 187 °C369 °FISO 11357-1/-3
UL RTI, Electrical 160 °C320 °F50% decrease of tensile strength after 20000h; 746B
Flammability, UL94  V-1
@Thickness 1.60 mm
V-1
@Thickness 0.0630 in
 V-0
@Thickness 3.20 mm
V-0
@Thickness 0.126 in
Oxygen Index 40 %40 %ISO 4589-1/-2
 
Processing PropertiesMetricEnglishComments
Melt Temperature 350 - 390 °C662 - 734 °FInjection molding
Mold Temperature 130 - 180 °C266 - 356 °FInjection molding
 
Descriptive Properties
ColorNatural and Black
Commercial StatusNorth America and Europe
Impact ModifiedNo
Primary Processing TechniqueInjection Molding and Extrution

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
BASF Ultrason® S 2010 G6 30% Glass Filled PSU
Envalior Durethan® ECO BKV 20 FN20 000000 Nylon 6 (PA6), 20% Glass Fiber Reinforced, Dry
BASF Ultrason® S 2010 PSU
BASF Ultrason® S 3010 PSU
BASF Ultrason® E 2010 G4 MR SW 15102 20% Glass Filled PESU

PBASF9406 / 85170

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.