MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Unitika A1030GFL PA6, 30% Glass Fiber Reinforced, Dry
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, 30% Glass Fiber Filled

Material Notes:

Information provided by Unitika Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.36 g/cc0.0491 lb/in³ISO 1183
Water Absorption 1.3 %
@Time 86400 sec
1.3 %
@Time 24.0 hour
ISO 62
Moisture Absorption at Equilibrium 2.0 %2.0 %50% RH; ISO 62
Linear Mold Shrinkage, Flow 0.0020 cm/cm
@Thickness 3.20 mm
0.0020 in/in
@Thickness 0.126 in
Linear Mold Shrinkage, Transverse 0.0070 cm/cm
@Thickness 3.20 mm
0.0070 in/in
@Thickness 0.126 in
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 120120ISO 2039
Tensile Strength at Break 170 MPa24700 psiISO 527-1/-2
Elongation at Break 3.1 %3.1 %ISO 527-1/-2
Tensile Modulus 9.60 GPa1390 ksiISO 527-1/-2
Flexural Strength 250 MPa36300 psiISO 178
Flexural Modulus 8.20 GPa1190 ksiISO 178
Charpy Impact Unnotched 7.00 J/cm²33.3 ft-lb/in²ISO 179-1
Charpy Impact, Notched 1.10 J/cm²5.23 ft-lb/in²ISO 179-1
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 2.00e+13 ohm-cm2.00e+13 ohm-cmIEC 60093
Dielectric Constant 3.3
@Frequency 1e+6 Hz
3.3
@Frequency 1e+6 Hz
IEC 60250
Dielectric Strength 42.1 kV/mm
@Thickness 1.00 mm
1070 kV/in
@Thickness 0.0394 in
IEC 60243-1
Dissipation Factor 0.022
@Frequency 1e+6 Hz
0.022
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index 550 V550 VIEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear 31.0 µm/m-°C17.2 µin/in-°FISO 11359-2
Deflection Temperature at 0.46 MPa (66 psi) 217 °C423 °FISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 203 °C397 °FISO 75-1/-2
Flammability, UL94 HB
@Thickness 0.750 mm
HB
@Thickness 0.0295 in
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 255 - 265 °C491 - 509 °F
Middle Barrel Temperature 250 - 260 °C482 - 500 °F
Front Barrel Temperature 230 - 240 °C446 - 464 °F
Nozzle Temperature 255 - 265 °C491 - 509 °F
Mold Temperature 80.0 - 100 °C176 - 212 °F
Back Pressure 3.00 - 5.00 MPa435 - 725 psi
 
Descriptive Properties
Primary Pressure80-90 MPa
Secondary Pressure60-80 MPa

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Avient OnForce™ LFT PP-30LGF/001 Natural Polypropylene Homopolymer (PP Homopolymer)
Unitika A1030GFL PA6, 30% Glass Fiber Reinforced, Conditioned
Overview of materials for Acetal Copolymer, Unreinforced
Radici Radiflam® A RV300AE (cond.) Nylon 66-30GF
GEHR Plastics PA 6.6-30GF Nylon 6.6, 30% Glass Fiber, Dry

PUNITIK811 / 177833

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.