MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Wolf Kunststoff ZEDEX® ZX-324V2T A3F PEEK, PTFE Modified
Categories: Polymer; Thermoplastic; Polyketone; Polyetheretherketone (PEEK); Polyetheretherketone, PEEK, PTFE-Filled

Material Notes: Reduced friction; High wear resistance; High elasticity; Stress resistant
Applications: Shipbuilding; Chemical Engineering; Automotive Technology; Machine Tools

Information provided by Zedex

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.33 g/cc0.0480 lb/in³ISO 1183
Water Absorption 0.10 %
@Temperature 23.0 °C
0.10 %
@Temperature 73.4 °F
RMC 93%; DIN EN ISO 62
Moisture Absorption at Equilibrium 0.50 %0.50 %DIN EN ISO 62
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 100100DIN 53505
Hardness, Shore D 8787DIN 53505
Ball Indentation Hardness 175 MPa25400 psiDIN 2039
Tensile Strength at Break 90.0 MPa13100 psiDIN EN ISO 527
Tensile Strength 92.0 MPa13300 psiDIN EN ISO 527
Tensile Strength, Yield 76.0 MPa11000 psiElastic Limit
 92.0 MPa13300 psiDIN EN ISO 527
Tensile Stress at Strain 26.0 MPa
@Strain 1 %,
Time 3.60e+6 sec
3770 psi
@Strain 1 %,
Time 1000 hour
DIN 53444
Elongation at Break 23.9 %23.9 %
 23.9 %23.9 %DIN EN ISO 527
Elongation at Yield 1.5 %1.5 %Elastic Yield Point
 6.9 %6.9 %DIN EN ISO 527
 6.9 %6.9 %Elongation at Maximum Force; DIN EN ISO 527
Tensile Modulus 3.50 GPa508 ksiDIN EN ISO 527
Flexural Strength 110 MPa16000 psiOuter Fiber Stress at 3.5% Outer Fiber Strain; DIN EN ISO 178
 127 MPa18400 psiDIN EN ISO 178
Flexural Modulus 3.90 GPa566 ksiDIN EN ISO 178
Flexural Strain at Yield 5.7 %5.7 %DIN EN ISO 178
Compressive Strain at Break 5.4 %5.4 %Nominal Compressive Strain at Compressive Strength; DIN EN ISO 604
Compressive Strain at Yield 5.4 %5.4 %Nominal; DIN EN ISO 604
Compressive Yield Strength 76.0 MPa11000 psiElastic Limit
 103 MPa14900 psiDIN EN ISO 604
Compressive Strength 103 MPa14900 psiDIN EN ISO 604
 35.0 MPa
@Time 3.60e+7 sec
5080 psi
@Time 10000 hour
 67.0 MPa
@Time 360000 sec
9720 psi
@Time 100 hour
 81.0 MPa
@Time 36.0 sec
11700 psi
@Time 0.0100 hour
 80.0 MPa
@Strain 3.5 %
11600 psi
@Strain 3.5 %
DIN EN ISO 604
Compressive Modulus 2.54 GPa368 ksiDIN EN ISO 604
Fatigue Strength 56.0 MPa
@# of Cycles 1.00e+6
8120 psi
@# of Cycles 1.00e+6
1 Hz
K Factor (ISO)  1.4 µm/km
@Temperature 100 °C
1.4 µm/km
@Temperature 212 °F
 4.8 µm/km
@Temperature 200 °C
4.8 µm/km
@Temperature 392 °F
 6.4 µm/km
@Temperature 240 °C
6.4 µm/km
@Temperature 464 °F
 12.1 µm/km
@Temperature 20.0 °C
12.1 µm/km
@Temperature 68.0 °F
Charpy Impact Unnotched NBNBEN ISO 179/1eU
Charpy Impact, Notched 0.630 J/cm²3.00 ft-lb/in²EN ISO 179/1eA
Coefficient of Friction, Dynamic  0.090
@Temperature 100 °C
0.090
@Temperature 212 °F
Dry Operation
 0.16
@Temperature 20.0 °C
0.16
@Temperature 68.0 °F
Dry Operation
Coefficient of Friction, Static 0.13
@Temperature 20.0 °C
0.13
@Temperature 68.0 °F
Dry Operation
Tensile Creep Modulus, 1000 hours 2500 MPa363000 psiAt 1% Deformation; DIN 53444
Limiting Pressure Velocity 0.46666 MPa-m/sec13323 psi-ft/minv = 100m/min
 0.500 MPa-m/sec14300 psi-ft/minv = 200m/min
 0.66666 MPa-m/sec19033 psi-ft/minv = 10m/min
 1.0355 MPa-m/sec29564 psi-ft/minv = 1m/min
Compression Set 3.3 %3.3 %Elastic Compression Limit
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 6.00e+16 ohm-cm6.00e+16 ohm-cmIEC 93
Surface Resistance 6.80e+12 ohm6.80e+12 ohmIEC 93
Dielectric Constant 3.3
@Frequency 110 Hz
3.3
@Frequency 110 Hz
IEC 250
Dielectric Strength 27.0 kV/mm686 kV/inIEC 243
Dissipation Factor 0.00200.0020IEC 112
 0.061
@Frequency 110 Hz
0.061
@Frequency 110 Hz
 
Thermal PropertiesMetricEnglishComments
CTE, linear  62.0 µm/m-°C
@Temperature <=100 °C
34.4 µin/in-°F
@Temperature <=212 °F
ISO E 830
 65.0 µm/m-°C
@Temperature <=150 °C
36.1 µin/in-°F
@Temperature <=302 °F
ISO E 831
Specific Heat Capacity 1.05 J/g-°C0.251 BTU/lb-°FDSC
Melting Point 340 °C644 °FDSC
Maximum Service Temperature, Air 115 °C239 °FPressed Bushings
 250 °C482 °FContinuous
 260 °C500 °FShort Term (3h)
Deflection Temperature at 1.8 MPa (264 psi) 171 °C340 °FDIN EN ISO 75
Glass Transition Temp, Tg 146 °C295 °FDSC
Flammability, UL94 V-0V-0
 
Compliance PropertiesMetricEnglishComments
FDA YesYes
 
Descriptive Properties
Alignment Adjustment4Nominal Scale: 1, low; 10, high
Chemical Sterilization10Nominal Scale: 1, low; 10, high
ColorBeige
Creep Resistance5Nominal Scale: 1, low; 10, high
Dimensional Stability with Thermal Expansion5Nominal Scale: 1, low; 10, high
Free from SiliconApplicable
Gamma-rays Radiation Sterilization7Nominal Scale: 1, low; 10, high
High Precision Bushings (negative clearance)Applicable
Injection Molded PartsApplicable
Machined PartsApplicable
Moist Heat Sterilization10Nominal Scale: 1, low; 10, high
Plastic GranulesApplicable
Resistance Against dust, Dirt, Abrasive Substances7Nominal Scale: 1, low; 10, high
Resistance Against Hot Water200
Resistance to Chemicals9Nominal Scale: 1, low; 10, high
Resistant Against DisinfectantApplicable
Rods up to Øe (de)Applicable
ROHS/WEEEApplicable
Sheets up to Maximum ThicknessApplicable
Sliding Velocity200
Suitable for Outdoor Use7Nominal Scale: 1, low; 10, high
Suitable for Use in WaterApplicable
Suitable for VacuumApplicable
Tubes (hollow rods) up to Øe (de)Applicable
UV Rays Resistance9Nominal Scale: 1, low; 10, high
UV-Sterilization7Nominal Scale: 1, low; 10, high

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Wolf Kunststoff ZEDEX® ZX-324 A3A PEEK
LATI Latilub 88/50-20T PEEK, PTFE Filled
Ensinger Tecapeek® XP-95 Compression Molded PEEK Compound, 15% PTFE Filled
VICTREX™ PEEK 450FE20 Polyetheretherketone, 20% PTFE
Wolf Kunststoff ZEDEX® ZX-324V11T A3L PEEK Polymer, Reinforced

PZEDEX07 / 122122

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.