MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Celanese Hytrel® HTR8206 TPC-ET
Categories: Polymer; Thermoplastic; Elastomer, TPE; Polyester TPE

Material Notes: High Performance Polyester Elastomer with High Moisture Vapor Transmission Rate Developed for Extrusion and Injection Molding

Former DuPont product acquired by Celanese in 2022.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.19 g/cc0.0430 lb/in³ISO 1183
Melt Density 1.02 g/cc
@Temperature 230 °C
0.0368 lb/in³
@Temperature 446 °F
Water Absorption 35 %
@Time 86400 sec
35 %
@Time 24.0 hour
Immersion; Sim. to ISO 62
Moisture Absorption 1.30 %
@Thickness 2.00 mm
1.30 %
@Thickness 0.0787 in
Sim. to ISO 62
Linear Mold Shrinkage, Flow 0.014 cm/cm0.014 in/inISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.015 cm/cm0.015 in/inISO 294-4, 2577
Melt Flow 14 g/10 min
@Load 2.16 kg,
Temperature 220 °C
14 g/10 min
@Load 4.76 lb,
Temperature 428 °F
14 cm³/10min Volumetric; ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 383815s; ISO 48-4
 <= 40<= 40ISO 48-4
Tensile Stress at Strain  3.40 MPa
@Strain 5.0 %
493 psi
@Strain 5.0 %
1BA specimen at 50mm/min; ISO 527-1/-2
 5.10 MPa
@Strain 10 %
740 psi
@Strain 10 %
ISO 527-1/-2
 9.50 MPa
@Strain 50 %
1380 psi
@Strain 50 %
ISO 527-1/-2
Tensile Modulus 0.0800 GPa11.6 ksiISO 527-1/-2
Flexural Modulus 0.0800 GPa11.6 ksiISO 178
Poissons Ratio 0.490.49
Charpy Impact Unnotched  NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
ISO 179/1eU
 NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
ISO 179/1eU
Charpy Impact, Notched  NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
ISO 179/1eA
 NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
ISO 179/1eA
 
Thermal PropertiesMetricEnglishComments
Specific Heat Capacity 2.10 J/g-°C
@Temperature 230 °C
0.502 BTU/lb-°F
@Temperature 446 °F
Melt
Thermal Conductivity 0.160 W/m-K
@Temperature 230 °C
1.11 BTU-in/hr-ft²-°F
@Temperature 446 °F
Melt
Melting Point 200 °C392 °F10°C/min; ISO 11357-1/-3
Flame Spread <= 80.0 mm/min
@Thickness 1.00 mm
<= 3.15 in/min
@Thickness 0.0394 in
ISO 3795 (FMVSS 302)
 
Processing PropertiesMetricEnglishComments
Melt Temperature 215 - 230 °C419 - 446 °FRange, Extrusion
 220 - 240 °C428 - 464 °FRange, Injection
 230 °C446 °FOptimum, Injection
Mold Temperature 45.0 °C113 °FOptimum, Injection
 40.0 - 50.0 °C104 - 122 °FInjection
Drying Temperature 100 °C212 °FInjection
 110 °C230 °FExtrusion
Dry Time 2.00 - 3.00 hour2.00 - 3.00 hourExtrusion, Dehumidified Dryer
 2.00 - 4.00 hour2.00 - 4.00 hourInjection, Dehumidified Dryer
Moisture Content <= 0.060 %<= 0.060 %Extrusion
 <= 0.080 %<= 0.080 %Injection
 
Descriptive Properties
Drying RecommendedyesInjection
Eff. thermal diffusivity (m²/s)5.44E-08DS
FMVSS ClassBISO 3795 (FMVSS 302)
Part Marking Code>TPC-ET<ISO 11469
PolymerTPC
Resin IdentificationTPC-ETISO 1043

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Celanese Hytrel® HTR8223 BK320 TPC-ET
DuPont Mobility and Materials Hytrel® HTR8139BK TPC-ET
Celanese Hytrel® 4556 TPC-ET
Celanese Hytrel® HTR8068 TPC-ET-FR(17)
Celanese Hytrel® 4068 TPC-ET

PDSX5210 / 197850

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.