MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Shinil Chemical SHINFLAME PC/ABS/GF Flame Retardant Polymer Housing
Categories: Polymer; Thermoplastic; ABS Polymer; Polycarbonate/ABS Alloy, Glass Fiber Filled; Polycarbonate (PC)

Material Notes: SHINFLAME is a flame retardant (FR) compound which exhibits inherent flame retardant properties during fire. Shinil uses its patented dispersion blending technology with variety of polymers to produce high performance SHINFLAME compound. SHINFLAME compounds comprise halogen or non halogen flame retardant additives in engineering thermoplastics. SHINFLAME provides a wide range of the flame performance (V0, V1, V2, HB etc), mechanical and physical properties to create the application-specific environment.

    Feature and Benefits
  • Excellent fire performance
  • Non halogen FR available
  • Environmentally friendly
  • RoHS compliance (selected grade)
  • Outstanding mechanical properties
  • Improved thermal properties
  • Easy processing
  • Non toxic

Information Provided by Shinil Chemical Industry Co., Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.42 g/cc1.42 g/cc
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 97.1 MPa14100 psi
Elongation at Break 4.0 %4.0 %
Flexural Strength 142.2 MPa20630 psi
Flexural Modulus 6.96 GPa1010 ksi
Izod Impact, Notched 0.883 J/cm1.65 ft-lb/in
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 135 °C275 °F
Flammability, UL94 V-0V-0

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Covestro Bayblend® T88-2N Polycarbonate + ABS, 10% Glass Filled
EPICHEM Epilon PC GF 10 V0 Polycarbonate, 10% Glass Fiber
Covestro Bayblend® T 88-2N Polycarbonate/ABS Blend, 10% Glass Fiber
Covestro Bayblend® T65 XF Polycarbonate + ABS
Celanese Zytel® 73G15HSL BK363 PA6-GF15

PSHINL30 / 104032

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.