MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

CeramTec DC 25 Dispersion Ceramic, Al2O3-ZrO2
Categories: Ceramic; Oxide; Aluminum Oxide

Material Notes: DC 25 is a ZTA Alumina Zirconia Platelet Composite used in dental applications.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 4.37 g/cc0.158 lb/in³DIN EN 623-2
Water Absorption 0.00 %0.00 %Open Porosity; DIN EN 623-2
Particle Size 0.54 µm0.54 µmGrain
Permeability 0.000.00%, Gas
Weibull Modulus 1414DINV ENV 843-5
 
Mechanical PropertiesMetricEnglishComments
Vickers Microhardness 19101910HV1; DINV ENV 843-4
Tensile Modulus 357 GPa51800 ksiYoung's; DINV ENV 843-2
Flexural Strength 1350 MPa196000 psiDIN EN 843-1
 1390 MPa202000 psiBending Strength; 4-Point; DIN ENV 843-1
Compressive Strength 4700 MPa682000 psiDIN 51067T1
Poissons Ratio 0.240.24DINV ENV 843-2
Fracture Toughness 6.40 MPa-m½5.82 ksi-in½KIC (SEVNB); DIN CEN/TS 14425-1
Shear Modulus 144 GPa20900 ksiCalculated
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 2000 ohm-cm2000 ohm-cmIEC 672-1
Dielectric Strength 16.5 kV/mm419 kV/inIEC 672-1
 
Thermal PropertiesMetricEnglishComments
CTE, linear 8.10 µm/m-°C
@Temperature 20.0 - 400 °C
4.50 µin/in-°F
@Temperature 68.0 - 752 °F
DIN EN 821-1
Specific Heat Capacity 0.700 J/g-°C0.167 BTU/lb-°FDINV ENV 821-3
Thermal Conductivity 17.0 W/m-K118 BTU-in/hr-ft²-°FDIN EN 821-2
Maximum Service Temperature, Air 1000 °C1830 °F
Maximum Service Temperature, Inert 1000 °C1830 °F
 
Component Elements PropertiesMetricEnglishComments
Al2O3 74 %74 %DIN EN ISO 12677
Cr2O3 0.30 %0.30 %DIN EN ISO 12677
Y2O3 0.60 %0.60 %DIN EN ISO 12677
ZrO2 24 %24 %DIN EN ISO 12677
 
Descriptive Properties
ColorMagenta
Monoclinic Content (%)< 10DIN EN ISO 12677
Other Oxides (%)< 0.1DIN EN ISO 12677
Ra = Arithmetic Mean Roughness Value (µm)<0.06
Radioactivity (Bq/kg)< 25
Thermal Shock Resistance R1 (K)355calculated; R1 = [σs (1-µ)] / (α·E)

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
CeramTec DN 70 Dispersion Ceramic, Al2O3-ZrO2
CeramTec 950 Zirconia Toughened Alumina (ZTA), Al2O3•ZrO2
CeramTec ZN 40 Zirconia, ZrO2-MgO
CeramTec B 40 Alumina, 99.1%
CeramTec 771 94% Alumina (Al2O3)

CCERA907 / 107507

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.