MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

LyondellBasell Moplen EP548P Polypropylene, Impact Modified; Molded/Extruded
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Impact Modified; Molded/Extruded

Material Notes: Moplen EP548P is a nucleated heterophasic copolymer, suitable for injection molding applications, and contains an anti-static agent. It exhibits a high stiffness combined with a medium fluidity. Moplen EP548P is extensively used in house ware, furniture, cylindrical containers and crates. Applications: Crates, Furniture, House wares, Opaque Containers.

Information provided by LyondellBasell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.900 g/cc0.0325 lb/in³ISO 1183-1
Melt Flow 16 g/10 min
@Load 2.16 kg,
Temperature 230 °C
16 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ISO 1133-1
 
Mechanical PropertiesMetricEnglishComments
Ball Indentation Hardness 69.0 MPa10000 psiISO 2039-1
Tensile Strength, Yield 28.0 MPa4060 psiISO 527-1,-2
Elongation at Break >= 50 %>= 50 %ISO 527-1,-2
Elongation at Yield 7.0 %7.0 %ASTM D638
Tensile Modulus 1.40 GPa203 ksiISO 527-1,-2
Charpy Impact, Notched  0.300 J/cm²
@Temperature -20.0 °C
1.43 ft-lb/in²
@Temperature -4.00 °F
Type 1, Edgewise, Notch A; ISO 179
 0.600 J/cm²
@Temperature 0.000 °C
2.86 ft-lb/in²
@Temperature 32.0 °F
Type 1, Edgewise, Notch A; ISO 179
 0.800 J/cm²
@Temperature 23.0 °C
3.81 ft-lb/in²
@Temperature 73.4 °F
Type 1, Edgewise, Notch A; ISO 179
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 100 °C212 °Funannealed; ISO 75B-1,-2
Vicat Softening Point 70.0 °C158 °FB50; ISO 306
 147 °C297 °FA50N; ISO 306
Brittleness Temperature -45.0 °C-49.0 °FISO 6603-2
 
Descriptive Properties
Processing MethodInjection Molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
LyondellBasell Moplen EP548Q Polypropylene, Impact Modified; Molded/Extruded
LyondellBasell Moplen EP548L Polypropylene, Impact Modified; Molded/Extruded
PolyMirae Moplen EP548P Injection Molding Grade Polypropylene
Teijin Panlite® L-1250J Polycarbonate, Hot Water Resistant Grade
LyondellBasell Moplen EP548S Polypropylene, Impact Modified; Molded/Extruded

PEQT8960 / 220594

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.