MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Envalior Arnitel® XG6029 TPC-ET
Categories: Polymer; Thermoplastic; Elastomer, TPE; Polyester TPE; Polyester, TP

Material Notes: Extrusion Grade

Former DSM Engineering Plastics product line is now with Envalior.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.13 g/cc0.0408 lb/in³ISO 1183
Water Absorption 0.20 %0.20 %Sim. To ISO 62
Moisture Absorption 0.640 %0.640 %Sim. To ISO 62
Melt Flow 4.0 g/10 min
@Load 2.16 kg,
Temperature 230 °C
4.0 g/10 min
@Load 4.76 lb,
Temperature 446 °F
cm3/10min Melt Volume-flow Rate; ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 88
@Time 3.00 sec
88
@Time 0.000833 hour
ISO 868
Hardness, Shore D 42
@Time 3.00 sec
42
@Time 0.000833 hour
ISO 868
Tensile Strength, Ultimate 9.70 MPa1410 psiISO 527-1/-2
Tensile Stress at Strain  2.60 MPa
@Strain 10 %
377 psi
@Strain 10 %
ISO 527-1/-2
 4.50 MPa
@Strain 100 %
653 psi
@Strain 100 %
ISO 527-1/-2
Elongation at Break 420 %420 %ISO 527-1/-2
Tensile Modulus 0.0450 GPa6.53 ksiISO 527-1/-2
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 8.30e+12 ohm-cm8.30e+12 ohm-cmIEC 60093
Dielectric Constant 3.53.5IEC 60250
 3.73.7IEC 60250
Dielectric Strength 19.7 kV/mm500 kV/inIEC 60243-1
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 180 µm/m-°C100 µin/in-°FISO 11359-1/-2
CTE, linear, Transverse to Flow 190 µm/m-°C106 µin/in-°FISO 11359-1/-2
Melting Point 180 °C356 °F10°C/min; ISO 11357-1/-3

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Envalior Arnitel® XG5857 TPC-ET
Toyobo PELPRENE™ P80C Polyester TPE, High Flexibility, High Melting Point
Toyobo PELPRENE™ P40H Polyester TPE
Overview of materials for Thermoplastic Polyurethane, Elastomer, Ether Grade
Overview of materials for Thermoplastic Olefinic Elastomer (TPO)

PDSM9801 / 161422

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.