MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Ineos H35G-00 Polypropylene Homopolymer  (discontinued **)
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Molded

Material Notes: This is a general purpose homopolymer for injection molding applications. This material meets the requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520.

    Applications
  • Consumer products
  • Housewares
  • Rigid packaging
  • Fiber
  • Extrusion coating

    Benefits
  • Easy moldability
  • Fast cycles at low processing temperatures

Information provided by Ineos Olefins & Polymers USA

Key Words: General purpose
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.902 g/cc0.0326 lb/in³ASTM D792
Melt Flow 35 g/10 min
@Load 2.16 kg,
Temperature 230 °C
35 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 103103Injection Molded; ASTM D785
Tensile Strength at Break 22.0 MPa3190 psi2.0 in/min, Injection Molded; ASTM D638
Tensile Strength, Yield 35.2 MPa5110 psi2.0 in/min, Injection Molded; ASTM D638
Elongation at Break <= 50 %<= 50 %2.0 in/min, Injection Molded; ASTM D638
Elongation at Yield 9.5 %9.5 %2.0 in/min, Injection Molded; ASTM D638
Flexural Modulus, 1% Secant 1490 MPa216000 psiInjection Molded; ASTM D790A
Izod Impact, Notched 0.240 J/cm0.450 ft-lb/inInjection Molded; ASTM D256
Izod Impact, Notched (ISO) 2.37 kJ/m²1.13 ft-lb/in²Area, Injection Molded; ASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 99.4 °C211 °FUnannealed, Injection Molded; ASTM D648
 
Optical PropertiesMetricEnglishComments
Haze 75 %
@Thickness 1.27 mm
75 %
@Thickness 0.0500 in
ASTM D1003
Gloss 95 %95 %60°; ASTM D2457
 
Compliance PropertiesMetricEnglishComments
FDA YesYesSee notes for details.
 
Descriptive Properties
ProcessInjection Molding

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Ineos H35G-GP Polypropylene Homopolymer
Ineos H02C-00 Polypropylene Homopolymer
Ineos 3950 Polypropylene Impact Copolymer
Ineos H20Z-03 Polypropylene Homopolymer
Ineos H35Z-00 Polypropylene Homopolymer

PINEOS045 / 99366

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.