MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Ferro Aluminum Oxide P99
Categories: Ceramic; Oxide; Aluminum Oxide

Material Notes: Manufactured at the Diamonite Plant in Shreve, Ohio. Data provided by the manufacturer, Ferro Corporation.

Key Words: Al2O3, alumina, aluminium oxide, aluminum oxide
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 3.90 - 3.94 g/cc0.141 - 0.142 lb/in³
Water Absorption 0.00 %0.00 %
Open Porosity 0.00 %0.00 %Gas tight. Test with helium mass spectrometer
Weibull Modulus 1010
 
Mechanical PropertiesMetricEnglishComments
Knoop Microhardness 14001400KHN5 microhardness, kg/mm²
Vickers Microhardness 15301530HV5 microhardness, kg/mm²
Tensile Strength, Ultimate 215 MPa31200 psiACMA Test #4
Modulus of Elasticity 331 GPa48000 ksiultrasonic
Compressive Strength 1800 MPa261000 psiASTM C773-74
Poissons Ratio 0.260.26ASTM C623
Fracture Toughness 4.30 MPa-m½3.91 ksi-in½Kic (indentation)
Shear Modulus 131 GPa19000 ksiultrasonic
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity  1.60e+7 ohm-cm
@Temperature 700 °C
1.60e+7 ohm-cm
@Temperature 1290 °F
ASTM D257
 5.50e+8 ohm-cm
@Temperature 500 °C
5.50e+8 ohm-cm
@Temperature 932 °F
ASTM D257
 2.50e+11 ohm-cm
@Temperature 300 °C
2.50e+11 ohm-cm
@Temperature 572 °F
ASTM D257
 1.50e+15 ohm-cm
@Temperature 100 °C
1.50e+15 ohm-cm
@Temperature 212 °F
ASTM D257
Dielectric Constant 9.8
@Frequency 1e+6 Hz
9.8
@Frequency 1e+6 Hz
ASTM D-116
Dielectric Strength 8.46 kV/mm
@Thickness 6.35 mm
215 kV/in
@Thickness 0.250 in
ASTM D149
Dissipation Factor 0.0020
@Frequency 1e+6 Hz
0.0020
@Frequency 1e+6 Hz
ASTM D-116
 
Thermal PropertiesMetricEnglishComments
CTE, linear  5.10 µm/m-°C
@Temperature 25.0 - 200 °C
2.83 µin/in-°F
@Temperature 77.0 - 392 °F
ASTM C32
 7.40 µm/m-°C
@Temperature 25.0 - 500 °C
4.11 µin/in-°F
@Temperature 77.0 - 932 °F
ASTM C32
 8.10 µm/m-°C
@Temperature 25.0 - 800 °C
4.50 µin/in-°F
@Temperature 77.0 - 1470 °F
 8.50 µm/m-°C
@Temperature 25.0 - 1000 °C
4.72 µin/in-°F
@Temperature 77.0 - 1830 °F
ASTM C32
Thermal Conductivity 35.4 W/m-K246 BTU-in/hr-ft²-°F
 5.40 W/m-K
@Temperature 1000 °C
37.5 BTU-in/hr-ft²-°F
@Temperature 1830 °F
 6.30 W/m-K
@Temperature 800 °C
43.7 BTU-in/hr-ft²-°F
@Temperature 1470 °F
 10.1 W/m-K
@Temperature 400 °C
70.1 BTU-in/hr-ft²-°F
@Temperature 752 °F
 
Component Elements PropertiesMetricEnglishComments
Al2O3 99.5 %99.5 %
 
Descriptive Properties
ColorOff White

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
GBC Grade 99 Alumina
Corundum, Aluminum Oxide, Alumina, 99.9%, Al2O3
Anderman Ceramics EA99P Sintered Alumina, 99%, Porous
CeramTec B 40 Alumina, 99.1%
Goodfellow Shapal™-M soft Aluminum Nitride (AlN) - Machinable

CFC012 / 810

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.