MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Mocom (ALBIS) ALTECH® PC A 2020/500 PC, 20% Glass Fiber Reinforced
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate, 20% Glass Filled

Material Notes: Base Polymer: Polycarbonate

Filler/Additive System: 20% glass fibers

Special Features: Heat ageing stabilization, injection molding grade, easy release (demolding)

Market Segment: Various

Application Area: Various

Information provided by Albis Plastics

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.33 g/cc0.0480 lb/in³ISO 1183
Maximum Moisture Content 0.0200.020
Melt Flow 19 g/10 min
@Load 1.20 kg,
Temperature 300 °C
19 g/10 min
@Load 2.65 lb,
Temperature 572 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 70.0 MPa10200 psiISO 527
Elongation at Break 3.3 %3.3 %ISO 527
Tensile Modulus 4.40 GPa638 ksiISO 527
Flexural Strength 110 MPa16000 psiISO 178
Flexural Modulus 4.20 GPa609 ksiISO 178
Charpy Impact Unnotched 4.50 J/cm²21.4 ft-lb/in²ISO 179/1eU
Charpy Impact, Notched 0.400 J/cm²1.90 ft-lb/in²ISO 179/1eA
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 138 °C280 °FISO 75-1/-2
Vicat Softening Point 145 °C293 °FB50; ISO 306
Flammability, UL94 V-2
@Thickness 1.50 mm
V-2
@Thickness 0.0591 in
 
Processing PropertiesMetricEnglishComments
Melt Temperature 310 - 330 °C590 - 626 °FInjection molding
Mold Temperature 80.0 - 130 °C176 - 266 °FInjection molding
Drying Temperature 120 °C
@Time 7200 - 14400 sec
248 °F
@Time 2.00 - 4.00 hour
in a dry air (desiccant) dryer
 
Descriptive Properties
Base PolymerPolycarbonate

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Mocom (ALBIS) ALTECH® PC ECO 2020/140 PC, 20% Glass Fiber Reinforced
Mocom (ALBIS) ALTECH® PC ECO 2020/146 FR GF20 PC, 20% Glass Fiber Reinforced
Eurotec® Tecotek® PC40 GR20 NL PC, 20% glass fiber reinforced, natural
LATI Latiohm 87/28-05 PD01 G/10 PC, 10% Glass Fiber Reinforced
Eurotec® Tecotek® PC43 GR20 BK002 PC, 20% glass fiber reinforced, black

PALBIS8798 / 242857

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.