MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

LATI Latiohm 87/28-05 PD01 G/10 PC, 10% Glass Fiber Reinforced
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate, 10% Glass Filled

Material Notes: Semiconductive/dissipative product based on Polycarbonate (PC). Glass fibers.

Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North America

Information provided by Lati Industria Termoplastici S.p.A.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.28 g/cc0.0462 lb/in³
Linear Mold Shrinkage, Flow 0.0020 - 0.0035 cm/cm0.0020 - 0.0035 in/in
Linear Mold Shrinkage, Transverse 0.0035 - 0.0055 cm/cm0.0035 - 0.0055 in/in
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 100 MPa14500 psi
Elongation at Break 1.8 %1.8 %
Tensile Modulus 7.50 GPa1090 ksi
Charpy Impact Unnotched 3.50 J/cm²16.7 ft-lb/in²
Charpy Impact, Notched 1.00 J/cm²4.76 ft-lb/in²
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 3000 ohm-cm3000 ohm-cm
Surface Resistance 2000 ohm2000 ohm
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 145 °C293 °F
Deflection Temperature at 1.8 MPa (264 psi) 140 °C284 °F
Vicat Softening Point 150 °C
@Load 5.00 kg
302 °F
@Load 11.0 lb
 
Processing PropertiesMetricEnglishComments
Melt Temperature 275 - 320 °C527 - 608 °F
Mold Temperature 100 - 120 °C212 - 248 °F
Drying Temperature 110 - 130 °C
@Time 10800 sec
230 - 266 °F
@Time 3.00 hour
 
Descriptive Properties
ISO Shrinkage - Pressure60 MPa

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Mocom (ALBIS) ALTECH® PC ECO 2010/121 GF10 IM UV PC, 10% Glass Fiber Reinforced
Mocom (ALBIS) ALTECH® PC A 2020/500 PC, 20% Glass Fiber Reinforced
LATI Latilon 30D G/10-V0 PC, 10% Glass Fiber Reinforced, Flame Retardant
RTP Company EMI 331 E FR Polycarbonate (PC) 10% Glass Fiber - Stainless Steel Fiber - Electrically Conductive - EMI/RFI/ESD Protection - Flame Retardant
Eurotec® Tecotek® PC43 GR10 BK002 PC, 10% glass fiber reinforced, black

PLATH9956 / 177652

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.