MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

INEOS Styrolution Lustran® 248 Acrylonitrile Butadiene Styrene (ABS)
Categories: Polymer; Thermoplastic; ABS Polymer; Acrylonitrile Butadiene Styrene (ABS), Molded

Material Notes: Lustran® 248 resin is a high-gloss, medium-impact grade of ABS (Acrylonitrile Butadiene Styrene). This general-purpose injection molding grade offers a good balance of physical properties. Features: High gloss, Good rigidity, Medium impact strength, UL94 HB rated. Applications: Toys, Small appliances

Information provided by Styrolution.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.06 g/cc0.0383 lb/in³ASTM D 792
Linear Mold Shrinkage 0.0040 - 0.0060 cm/cm0.0040 - 0.0060 in/inASTM D 955
Melt Flow  5.0 g/10 min
@Load 3.80 kg,
Temperature 230 °C
5.0 g/10 min
@Load 8.38 lb,
Temperature 446 °F
ASTM D 1238
 13 g/10 min
@Load 10.0 kg,
Temperature 220 °C
13 g/10 min
@Load 22.0 lb,
Temperature 428 °F
ASTM D 1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 112112ASTM D 785
Tensile Strength, Yield 46.9 MPa6800 psiASTM D 638
Tensile Modulus 2.62 GPa380 ksiASTM D 638
Flexural Strength 38.0 MPa5510 psiASTM D 790
Flexural Yield Strength 73.8 MPa
@Strain 5.0 %
10700 psi
@Strain 5.0 %
ASTM D 790
Izod Impact, Notched  0.481 J/cm
@Temperature -40.0 °C
0.900 ft-lb/in
@Temperature -40.0 °F
ASTM 256
 2.24 J/cm
@Temperature 23.0 °C
4.20 ft-lb/in
@Temperature 73.4 °F
ASTM 256
 
Thermal PropertiesMetricEnglishComments
CTE, linear 81.0 µm/m-°C45.0 µin/in-°FASTM D 696
Deflection Temperature at 0.46 MPa (66 psi) 93.0 °C199 °Funannealed; ASTM D 648
 100 °C212 °Fannealed; ASTM D 648
Deflection Temperature at 1.8 MPa (264 psi) 86.0 °C187 °Funannealed; ASTM D 648
 95.5 °C204 °Fannealed; ASTM D 648
Vicat Softening Point 107 °C
@Load 1.02 kg
225 °F
@Load 2.25 lb
B/2 120C/H; ASTM D 1525
 
Processing PropertiesMetricEnglishComments
Drying Temperature 79.0 °C
@Time 7200 - 14400 sec
174 °F
@Time 2.00 - 4.00 hour

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
INEOS Styrolution Lustran® 348 Acrylonitrile Butadiene Styrene (ABS)
Lotte Advanced Materials Starex® HG-0760GP ABS
LyondellBasell Pro-fax PD702 Polypropylene Homopolymer, High Flow
A. Schulman Matrixx 15A4201 Flame Retardant 20% Talc Filled Polypropylene (5VA)
A. Schulman Matrixx 12N4003 Polypropylene, FR

PSTYR9896 / 216123

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.