MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

BASF Ultradur® LUX PBT
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT)

Material Notes: The new Ultradur® LUX is a polybutylene terephthalate (PBT). Researchers at BASF have successfully refined its morphology so that its laser transparency has been improved from 30 to around 60 percent – a high, consistent laser transparency that has not previously been achieved with PBT. Its mechanical properties are comparable to those of standard Ultradur®. With the improved laser transparency it is now possible to achieve much higher welding speeds.

Information provided by BASF

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Optical PropertiesMetricEnglishComments
Transmission, Visible  40 %
@Wavelength 700 nm
40 %
@Wavelength 700 nm
 40 %
@Wavelength 2300 nm
40 %
@Wavelength 2300 nm
 60 %
@Wavelength 1700 nm
60 %
@Wavelength 1700 nm
 65 %
@Wavelength 2100 nm
65 %
@Wavelength 2100 nm
 70 %
@Wavelength 1300 nm
70 %
@Wavelength 1300 nm
 
Descriptive Properties
Commercial StatusEurope

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
BASF Ultrason® E 1010 PES
BASF Ultrason® E 2010 G4 MR SW 15102 20% Glass Filled PESU
BASF Ultrason® E 6020 P PES
CENTROPLAST CENTRO HPM Polysulfone
BASF Ultrason® S 2010 PSU

PBASG0117 / 131751

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.